3M™ Glass Cloth Tape 398FR has an acrylic adhesive for many applications requiring high adhesion, an abrasion-resistant backing and flame retardant properties. This product is typically used for sealing aircraft cargo bay panels to provide a permanent seal.Information provided by 3M |