MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 32664 Light Gray Heavy Duty Performance Coating - Part B
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and adhesion to metal, fiberglass, aluminum, wood (plywood, OSB, etc.), concrete and masonry. It is a two component 1:1 by volume system with adhesion enhancement chemical complexes. The protective coating can be applied up to 500mil thick and offers an ultra-fast cure that speeds production in an OEM setting. This aromatic formulation displays excellent chemical and environmental resistance while reducing the moisture problem that causes bubbling. It also offers high elongation and flexibility the produces high impact resistance.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 - 1.08 g/cc0.0365 - 0.0390 lb/in³
Solids Content 100 %100 %
Water Absorption <= 1.78 %<= 1.78 %ASTM D570
Brookfield Viscosity 150 - 1250 cP150 - 1250 cPRVT Model, Spindle #3 @ 20 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 54 - 6054 - 60ASTM D2240
Tensile Strength at Break 12.4 - 15.2 MPa1800 - 2200 psiASTM 638-01
Elongation at Break 93 %93 %ASTM 638-01
Tear Strength 49.9 - 58.6 kN/m285 - 335 pliASTM D624
Taber Abrasion, mg/1000 Cycles 35 - 4035 - 40ASTM D40695
Tangent Modulus 110 - 124 MPa16000 - 18000 psiTangent; ASTM 638-01
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °F
Minimum Service Temperature, Air -29.0 °C-20.2 °F
Flash Point 93.0 °C199 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 - 120 min1.00 - 2.00 hourlight use
 1440 min24.0 hourheavy duty use
Shelf Life 12.0 Month
@Temperature 21.0 - 32.0 °C
12.0 Month
@Temperature 69.8 - 89.6 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 398FR Glass Cloth Tape
Permabond UV640 UV-curable Adhesive
Momentive Performance Materials RTV112 One Component Acetoxy Adhesive Sealant, White
Master Bond EP21TDCF-3 Two Component, Higher Viscosity Epoxy System
Henkel Loctite® Ultra Grey® 5999 Flange Sealant

PMM34313 / 169060

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.