MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 398FR Glass Cloth Tape
Categories: Polymer; Tape

Material Notes: 3M™ Glass Cloth Tape 398FR has an acrylic adhesive for many applications requiring high adhesion, an abrasion-resistant backing and flame retardant properties. This product is typically used for sealing aircraft cargo bay panels to provide a permanent seal.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 127 microns5.00 milBacking; ASTM D3752
 178 microns7.00 milTotal; ASTM D3752
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 126.4 MPa18330 psiASTM D3759
Elongation at Break 7.0 %7.0 %ASTM D3759
Peel Strength 0.4163 kN/m2.375 pliAdhesion to Steel; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -29.0 °C-20.2 °F
 
Descriptive Properties
Adhesive TypeAcrylic
AppearanceWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nickel, Ni
3M 32664 Light Gray Heavy Duty Performance Coating - Part B
Overview of materials for Thermoset Polyurethane, Liquid
Overview of materials for Nylon 66, Aramid Fiber Filled
Lead, Pb

PMM34480 / 169227

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.