MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AK Steel TRAN-COR® H-2 CARLITE® Grain Oriented Electrical Steel (Extended Electro-Magnetic Data)
Categories: Metal; Electronic/Magnetic Alloy; Ferrous Metal

Material Notes: TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for lower core losses and less noisy transformer core structures, particularly at higher operating inductions, when compared to conventional grain oriented electrical steels. The core loss characteristics are further enhanced in the TRAN-COR H CARLITE DR® (Domain Refined) products where laser scribing is employed. In this process, a precisely focused laser beam is rapidly scanned across the steel surface. The micro-strain imparted into the material forces the pre-existing magnetic domains to subdivide. The finer domain structure reduces the distance that the domain walls must move during AC magnetization, thereby reducing eddy current losses. The result is far lower core loss than possible with conventional grain oriented electrical steels of comparable thickness. TRAN-COR H CARLITE products are suitable for all types of transformers while TRAN-COR H DR products are suitable for those types of transformers where a stress relief annealing treatment of the magnetic core is not used. Stress relief annealing will result in the eradication of the effect provided by the laser treatment and will result in a significant increase in core loss.

Information provided by AK Steel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.65 g/cc
Thickness 270 - 310 microns
 300 micronsNominal
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 173
Hardness, Rockwell B 83
Tensile Strength, Ultimate 359 MPaIn rolling direction
Tensile Strength, Yield 345 MPaIn rolling direction
Elongation at Break 11 %In 2", rolling direction
Modulus of Elasticity 113.8 GPaIn rolling direction
 138 GPaAt 20° to rolling direction
 203 GPaAt 90° to rolling direction
 241 GPaAt 45° to rolling direction
 276 GPaAt 55° to rolling direction
 
Electrical PropertiesOriginal ValueComments
Exciting Power (RMS) 0.00310 RMS VA/lb
@Magnetic Field 0.100 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.00340 RMS VA/lb
@Magnetic Field 0.100 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.00400 RMS VA/lb
@Magnetic Field 0.100 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.00430 RMS VA/lb
@Magnetic Field 0.100 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.0110 RMS VA/lb
@Magnetic Field 0.200 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.0114 RMS VA/lb
@Magnetic Field 0.200 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.0141 RMS VA/lb
@Magnetic Field 0.200 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.0147 RMS VA/lb
@Magnetic Field 0.200 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.0228 RMS VA/lb
@Magnetic Field 0.300 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.0233 RMS VA/lb
@Magnetic Field 0.300 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.0294 RMS VA/lb
@Magnetic Field 0.300 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.0300 RMS VA/lb
@Magnetic Field 0.300 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.0378 RMS VA/lb
@Magnetic Field 0.400 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.0381 RMS VA/lb
@Magnetic Field 0.400 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.0488 RMS VA/lb
@Magnetic Field 0.400 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.0492 RMS VA/lb
@Magnetic Field 0.400 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.0554 RMS VA/lb
@Magnetic Field 0.500 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.0556 RMS VA/lb
@Magnetic Field 0.500 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.0717 RMS VA/lb
@Magnetic Field 0.500 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.0720 RMS VA/lb
@Magnetic Field 0.500 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.0755 RMS VA/lb
@Magnetic Field 0.600 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.0755 RMS VA/lb
@Magnetic Field 0.600 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.0977 RMS VA/lb
@Magnetic Field 0.600 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.0977 RMS VA/lb
@Magnetic Field 0.700 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.0977 RMS VA/lb
@Magnetic Field 0.600 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.0977 RMS VA/lb
@Magnetic Field 0.700 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.1223 RMS VA/lb
@Magnetic Field 0.800 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.1227 RMS VA/lb
@Magnetic Field 0.800 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.1268 RMS VA/lb
@Magnetic Field 0.700 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.1273 RMS VA/lb
@Magnetic Field 0.700 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.1491 RMS VA/lb
@Magnetic Field 0.900 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.150 RMS VA/lb
@Magnetic Field 0.900 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.1591 RMS VA/lb
@Magnetic Field 0.800 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.160 RMS VA/lb
@Magnetic Field 0.800 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.1791 RMS VA/lb
@Magnetic Field 1.00 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.180 RMS VA/lb
@Magnetic Field 1.00 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.195 RMS VA/lb
@Magnetic Field 0.900 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.1959 RMS VA/lb
@Magnetic Field 0.900 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.2114 RMS VA/lb
@Magnetic Field 1.10 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.2132 RMS VA/lb
@Magnetic Field 1.10 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.2341 RMS VA/lb
@Magnetic Field 1.00 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.2355 RMS VA/lb
@Magnetic Field 1.00 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.2473 RMS VA/lb
@Magnetic Field 1.20 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.2495 RMS VA/lb
@Magnetic Field 1.20 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.2768 RMS VA/lb
@Magnetic Field 1.10 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.2791 RMS VA/lb
@Magnetic Field 1.10 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.2877 RMS VA/lb
@Magnetic Field 1.30 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.290 RMS VA/lb
@Magnetic Field 1.30 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.3241 RMS VA/lb
@Magnetic Field 1.20 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.3273 RMS VA/lb
@Magnetic Field 1.20 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.3327 RMS VA/lb
@Magnetic Field 1.40 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.3368 RMS VA/lb
@Magnetic Field 1.40 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.3773 RMS VA/lb
@Magnetic Field 1.30 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.3805 RMS VA/lb
@Magnetic Field 1.30 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.3891 RMS VA/lb
@Magnetic Field 1.50 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.3941 RMS VA/lb
@Magnetic Field 1.50 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.4364 RMS VA/lb
@Magnetic Field 1.40 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.4418 RMS VA/lb
@Magnetic Field 1.40 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.4655 RMS VA/lb
@Magnetic Field 1.60 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.4723 RMS VA/lb
@Magnetic Field 1.60 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.5091 RMS VA/lb
@Magnetic Field 1.50 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.5155 RMS VA/lb
@Magnetic Field 1.50 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.5959 RMS VA/lb
@Magnetic Field 1.70 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.6041 RMS VA/lb
@Magnetic Field 1.70 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.605 RMS VA/lb
@Magnetic Field 1.60 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.6141 RMS VA/lb
@Magnetic Field 1.60 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.765 RMS VA/lb
@Magnetic Field 1.70 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.7755 RMS VA/lb
@Magnetic Field 1.70 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.9864 RMS VA/lb
@Magnetic Field 1.80 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.9864 RMS VA/lb
@Magnetic Field 1.80 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 1.2318 RMS VA/lb
@Magnetic Field 1.80 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 1.2318 RMS VA/lb
@Magnetic Field 1.80 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 4.2545 RMS VA/lb
@Magnetic Field 1.90 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 4.2636 RMS VA/lb
@Magnetic Field 1.90 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 5.2818 RMS VA/lb
@Magnetic Field 1.90 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 5.2818 RMS VA/lb
@Magnetic Field 1.90 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
Electrical Resistivity 0.0000500 ohm-cm
 
Magnetic PropertiesOriginal ValueComments
Core Loss 0.00423 W/kg
@Magnetic Field 0.100 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.00436 W/kg
@Magnetic Field 0.100 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.00569 W/kg
@Magnetic Field 0.100 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.00586 W/kg
@Magnetic Field 0.100 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.01586 W/kg
@Magnetic Field 0.200 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.01613 W/kg
@Magnetic Field 0.200 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.0214 W/kg
@Magnetic Field 0.200 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.0218 W/kg
@Magnetic Field 0.200 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.0343 W/kg
@Magnetic Field 0.300 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.0350 W/kg
@Magnetic Field 0.300 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.0372 W/kg
@Magnetic Field 0.500 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.0463 W/kg
@Magnetic Field 0.300 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.0472 W/kg
@Magnetic Field 0.300 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.0593 W/kg
@Magnetic Field 0.400 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.0603 W/kg
@Magnetic Field 0.400 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.0799 W/kg
@Magnetic Field 0.400 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.0812 W/kg
@Magnetic Field 0.400 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.0917 W/kg
@Magnetic Field 0.500 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.1211 W/kg
@Magnetic Field 0.500 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.1232 W/kg
@Magnetic Field 0.500 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.1267 W/kg
@Magnetic Field 0.600 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.1288 W/kg
@Magnetic Field 0.600 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.1687 W/kg
@Magnetic Field 0.700 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.1699 W/kg
@Magnetic Field 0.600 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.1717 W/kg
@Magnetic Field 0.700 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.1727 W/kg
@Magnetic Field 0.600 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.216 W/kg
@Magnetic Field 0.800 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.220 W/kg
@Magnetic Field 0.800 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.226 W/kg
@Magnetic Field 0.700 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.230 W/kg
@Magnetic Field 0.700 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.269 W/kg
@Magnetic Field 0.900 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.275 W/kg
@Magnetic Field 0.900 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.289 W/kg
@Magnetic Field 0.800 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.295 W/kg
@Magnetic Field 0.800 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.329 W/kg
@Magnetic Field 1.00 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.337 W/kg
@Magnetic Field 1.00 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.360 W/kg
@Magnetic Field 0.900 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.368 W/kg
@Magnetic Field 0.900 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.395 W/kg
@Magnetic Field 1.10 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.405 W/kg
@Magnetic Field 1.10 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.439 W/kg
@Magnetic Field 1.00 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.450 W/kg
@Magnetic Field 1.00 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.468 W/kg
@Magnetic Field 1.20 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.479 W/kg
@Magnetic Field 1.20 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.527 W/kg
@Magnetic Field 1.10 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.540 W/kg
@Magnetic Field 1.10 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.548 W/kg
@Magnetic Field 1.30 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.561 W/kg
@Magnetic Field 1.30 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.625 W/kg
@Magnetic Field 1.20 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.636 W/kg
@Magnetic Field 1.40 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.640 W/kg
@Magnetic Field 1.20 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.650 W/kg
@Magnetic Field 1.40 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.732 W/kg
@Magnetic Field 1.30 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.737 W/kg
@Magnetic Field 1.50 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.740 W/kg
@Magnetic Field 1.50 T,
Frequency 50 Hz
Typical
 0.748 W/kg
@Magnetic Field 1.30 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.750 W/kg
@Magnetic Field 1.50 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.846 W/kg
@Magnetic Field 1.60 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.849 W/kg
@Magnetic Field 1.40 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.864 W/kg
@Magnetic Field 1.60 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 0.868 W/kg
@Magnetic Field 1.40 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 0.980 W/kg
@Magnetic Field 1.50 T,
Frequency 60 Hz
Typical
 0.982 W/kg
@Magnetic Field 1.50 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 0.990 W/kg
@Magnetic Field 1.70 T,
Frequency 50 Hz
Typical
 0.992 W/kg
@Magnetic Field 1.70 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 0.999 W/kg
@Magnetic Field 1.50 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 1.007 W/kg
@Magnetic Field 1.70 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 1.05 W/kg
@Magnetic Field 1.70 T,
Frequency 50 Hz
Maximum
 1.126 W/kg
@Magnetic Field 1.60 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 1.149 W/kg
@Magnetic Field 1.60 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 1.222 W/kg
@Magnetic Field 1.80 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 1.245 W/kg
@Magnetic Field 1.80 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 1.31 W/kg
@Magnetic Field 1.70 T,
Frequency 60 Hz
Typical
 1.313 W/kg
@Magnetic Field 1.70 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 1.333 W/kg
@Magnetic Field 1.70 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 1.40 W/kg
@Magnetic Field 1.70 T,
Frequency 60 Hz
Maximum
 1.596 W/kg
@Magnetic Field 1.80 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 1.629 W/kg
@Magnetic Field 1.80 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 1.718 W/kg
@Magnetic Field 1.90 T,
Frequency 50 Hz
ASTM A804, 0.30 mm
 1.746 W/kg
@Magnetic Field 1.90 T,
Frequency 50 Hz
ASTM A343, 0.30 mm
 2.22 W/kg
@Magnetic Field 1.90 T,
Frequency 60 Hz
ASTM A804, 0.30 mm
 2.26 W/kg
@Magnetic Field 1.90 T,
Frequency 60 Hz
ASTM A343, 0.30 mm
 
Descriptive Properties
Approximate Equivalent International GradeM105-30P5
Magnetostriction 10^8-45ASTM A876, 1.4T, 60Hz, 0.30 mm
 -48ASTM A876, 1.5T, 60Hz, 0.30 mm
 -53ASTM A876, 1.6T, 60Hz, 0.30 mm
 -55ASTM A876, 1.7T, 60Hz, 0.30 mm
Maximum Induction at 800 A/m (T)1.9
Minimum Lamination Factor (%)95.5
Typical Induction at 800 A/m (T)1.92
Typical Lamination Factor (%)97.3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel DI-MAX® HF-10 Nonoriented Electrical Steel (Extended Electrical/Magnetic Data)
AK Steel DI-MAX® HF-10 Nonoriented Electrical Steel
AK Steel DI-MAX® M-19 Nonoriented Electrical Steel
AK Steel CARLITE® M-6 Grain Oriented Electrical Steel
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel (Extended Electro-Magnetic Data)

NAKS165a / 140773

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.