MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AK Steel DI-MAX® HF-10 Nonoriented Electrical Steel
Categories: Metal; Electronic/Magnetic Alloy; Ferrous Metal

Material Notes: DI-MAX HF-10 is a fully processed nonoriented electrical steel designed for use in high speed motors, traction motors, aircraft generators, and other rotating equipment operating at frequencies above 60 Hz. DI-MAX HF-10 Electrical Steel is supplied in a nominal thickness of 0.25 mm (0.010 in).

Information provided by AK Steel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.65 g/cc0.276 lb/in³ASTM A34
Thickness 250 microns9.84 milAim
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7878
Tensile Strength, Ultimate 450 MPa65300 psi
Tensile Strength, Yield 350 MPa50800 psi
Elongation at Break 20 %20 %In 2"
 
Electrical PropertiesMetricEnglishComments
Exciting Power  0.0226 VA/lb
@Magnetic Field 0.100 T,
Frequency 50 Hz
0.0226 VA/lb
@Magnetic Field 0.100 T,
Frequency 50 Hz
ASTM A343, ASTM A348, 50/50, As-Sheared
 297.27 VA/lb
@Magnetic Field 1.70 T,
Frequency 200 Hz
297.27 VA/lb
@Magnetic Field 1.70 T,
Frequency 200 Hz
ASTM A343, ASTM A348, 50/50, Stress Relief Annealed
Electrical Resistivity 0.0000540 - 0.0000560 ohm-cm0.0000540 - 0.0000560 ohm-cm
 
Magnetic PropertiesMetricEnglishComments
Core Loss  0.0123 W/kg
@Magnetic Field 0.100 T,
Frequency 50 Hz
0.00558 W/lb
@Magnetic Field 0.100 T,
Frequency 50 Hz
ASTM A343, ASTM A348, 50/50, As-Sheared
 843 W/kg
@Magnetic Field 1.00 T,
Frequency 5000 Hz
382 W/lb
@Magnetic Field 1.00 T,
Frequency 5000 Hz
ASTM A343, ASTM A348, 50/50, Stress Relief Annealed
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.70 %0.70 %
Iron, Fe 96.65 %96.65 %As Balance
Silicon, Si 2.65 %2.65 %
 
Descriptive Properties
Magnetic Induction at 5000 A/m (T)1.65
Saturation Induction (T)1.99

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AK Steel DI-MAX® HF-10 Nonoriented Electrical Steel (Extended Electrical/Magnetic Data)
AK Steel DI-MAX® M-15 Nonoriented Electrical Steel
AK Steel DI-MAX® M-19 Nonoriented Electrical Steel
AK Steel DI-MAX® M-47 Nonoriented Electrical Steel
AK Steel DI-MAX® M-36 Nonoriented Electrical Steel

NAKS162a / 140766

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.