MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AK Steel TRAN-COR® H-1 CARLITE® DR® Grain Oriented Electrical Steel
Categories: Metal; Electronic/Magnetic Alloy; Ferrous Metal

Material Notes: TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for lower core losses and less noisy transformer core structures, particularly at higher operating inductions, when compared to conventional grain oriented electrical steels. The core loss characteristics are further enhanced in the TRAN-COR H CARLITE DR® (Domain Refined) products where laser scribing is employed. In this process, a precisely focused laser beam is rapidly scanned across the steel surface. The micro-strain imparted into the material forces the pre-existing magnetic domains to subdivide. The finer domain structure reduces the distance that the domain walls must move during AC magnetization, thereby reducing eddy current losses. The result is far lower core loss than possible with conventional grain oriented electrical steels of comparable thickness. TRAN-COR H CARLITE products are suitable for all types of transformers while TRAN-COR H DR products are suitable for those types of transformers where a stress relief annealing treatment of the magnetic core is not used. Stress relief annealing will result in the eradication of the effect provided by the laser treatment and will result in a significant increase in core loss.

Information provided by AK Steel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.65 g/cc0.276 lb/in³
Thickness 240 - 280 microns9.45 - 11.0 mil
 270 microns10.6 milNominal
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 173173
Hardness, Rockwell B 8383
Tensile Strength, Ultimate 359 MPa52100 psiIn rolling direction
Tensile Strength, Yield 345 MPa50000 psiIn rolling direction
Elongation at Break 11 %11 %In 2", rolling direction
Modulus of Elasticity 113.8 GPa16510 ksiIn rolling direction
 138 GPa20000 ksiAt 20° to rolling direction
 203 GPa29400 ksiAt 90° to rolling direction
 241 GPa35000 ksiAt 45° to rolling direction
 276 GPa40000 ksiAt 55° to rolling direction
 
Electrical PropertiesMetricEnglishComments
Exciting Power (RMS)  0.00158 RMS AT/cm
@Magnetic Field 0.100 T,
Frequency 50 Hz
0.00250 RMS VA/lb
@Magnetic Field 0.100 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.00196 RMS AT/cm
@Magnetic Field 0.100 T,
Frequency 60 Hz
0.00310 RMS VA/lb
@Magnetic Field 0.100 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.00550 RMS AT/cm
@Magnetic Field 0.200 T,
Frequency 50 Hz
0.00870 RMS VA/lb
@Magnetic Field 0.200 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.00702 RMS AT/cm
@Magnetic Field 0.200 T,
Frequency 60 Hz
0.0111 RMS VA/lb
@Magnetic Field 0.200 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.0116 RMS AT/cm
@Magnetic Field 0.300 T,
Frequency 50 Hz
0.0184 RMS VA/lb
@Magnetic Field 0.300 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.0149 RMS AT/cm
@Magnetic Field 0.300 T,
Frequency 60 Hz
0.0235 RMS VA/lb
@Magnetic Field 0.300 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.0196 RMS AT/cm
@Magnetic Field 0.400 T,
Frequency 50 Hz
0.0310 RMS VA/lb
@Magnetic Field 0.400 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.0251 RMS AT/cm
@Magnetic Field 0.400 T,
Frequency 60 Hz
0.0397 RMS VA/lb
@Magnetic Field 0.400 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.0292 RMS AT/cm
@Magnetic Field 0.500 T,
Frequency 50 Hz
0.0461 RMS VA/lb
@Magnetic Field 0.500 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.0376 RMS AT/cm
@Magnetic Field 0.500 T,
Frequency 60 Hz
0.0594 RMS VA/lb
@Magnetic Field 0.500 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.0403 RMS AT/cm
@Magnetic Field 0.600 T,
Frequency 50 Hz
0.0637 RMS VA/lb
@Magnetic Field 0.600 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.0520 RMS AT/cm
@Magnetic Field 0.600 T,
Frequency 60 Hz
0.0822 RMS VA/lb
@Magnetic Field 0.600 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.0531 RMS AT/cm
@Magnetic Field 0.700 T,
Frequency 50 Hz
0.0839 RMS VA/lb
@Magnetic Field 0.700 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.06757 RMS AT/cm
@Magnetic Field 0.800 T,
Frequency 50 Hz
0.1068 RMS VA/lb
@Magnetic Field 0.800 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.06846 RMS AT/cm
@Magnetic Field 0.700 T,
Frequency 60 Hz
0.1082 RMS VA/lb
@Magnetic Field 0.700 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.08396 RMS AT/cm
@Magnetic Field 0.900 T,
Frequency 50 Hz
0.1327 RMS VA/lb
@Magnetic Field 0.900 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.08712 RMS AT/cm
@Magnetic Field 0.800 T,
Frequency 60 Hz
0.1377 RMS VA/lb
@Magnetic Field 0.800 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.1033 RMS AT/cm
@Magnetic Field 1.00 T,
Frequency 50 Hz
0.1632 RMS VA/lb
@Magnetic Field 1.00 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.1084 RMS AT/cm
@Magnetic Field 0.900 T,
Frequency 60 Hz
0.1714 RMS VA/lb
@Magnetic Field 0.900 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.1262 RMS AT/cm
@Magnetic Field 1.10 T,
Frequency 50 Hz
0.1995 RMS VA/lb
@Magnetic Field 1.10 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.1332 RMS AT/cm
@Magnetic Field 1.00 T,
Frequency 60 Hz
0.2105 RMS VA/lb
@Magnetic Field 1.00 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.1536 RMS AT/cm
@Magnetic Field 1.20 T,
Frequency 50 Hz
0.2427 RMS VA/lb
@Magnetic Field 1.20 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.1625 RMS AT/cm
@Magnetic Field 1.10 T,
Frequency 60 Hz
0.2568 RMS VA/lb
@Magnetic Field 1.10 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.1870 RMS AT/cm
@Magnetic Field 1.30 T,
Frequency 50 Hz
0.2955 RMS VA/lb
@Magnetic Field 1.30 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.1970 RMS AT/cm
@Magnetic Field 1.20 T,
Frequency 60 Hz
0.3114 RMS VA/lb
@Magnetic Field 1.20 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.2269 RMS AT/cm
@Magnetic Field 1.40 T,
Frequency 50 Hz
0.3586 RMS VA/lb
@Magnetic Field 1.40 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.2384 RMS AT/cm
@Magnetic Field 1.30 T,
Frequency 60 Hz
0.3768 RMS VA/lb
@Magnetic Field 1.30 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.2743 RMS AT/cm
@Magnetic Field 1.50 T,
Frequency 50 Hz
0.4336 RMS VA/lb
@Magnetic Field 1.50 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.2873 RMS AT/cm
@Magnetic Field 1.40 T,
Frequency 60 Hz
0.4541 RMS VA/lb
@Magnetic Field 1.40 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.3342 RMS AT/cm
@Magnetic Field 1.60 T,
Frequency 50 Hz
0.5282 RMS VA/lb
@Magnetic Field 1.60 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.3451 RMS AT/cm
@Magnetic Field 1.50 T,
Frequency 60 Hz
0.5455 RMS VA/lb
@Magnetic Field 1.50 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.4179 RMS AT/cm
@Magnetic Field 1.60 T,
Frequency 60 Hz
0.6605 RMS VA/lb
@Magnetic Field 1.60 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.4388 RMS AT/cm
@Magnetic Field 1.70 T,
Frequency 50 Hz
0.6936 RMS VA/lb
@Magnetic Field 1.70 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.5427 RMS AT/cm
@Magnetic Field 1.70 T,
Frequency 60 Hz
0.8577 RMS VA/lb
@Magnetic Field 1.70 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.759 RMS AT/cm
@Magnetic Field 1.80 T,
Frequency 50 Hz
1.20 RMS VA/lb
@Magnetic Field 1.80 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.92317 RMS AT/cm
@Magnetic Field 1.80 T,
Frequency 60 Hz
1.4591 RMS VA/lb
@Magnetic Field 1.80 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 2.6372 RMS AT/cm
@Magnetic Field 1.90 T,
Frequency 50 Hz
4.1682 RMS VA/lb
@Magnetic Field 1.90 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 3.2067 RMS AT/cm
@Magnetic Field 1.90 T,
Frequency 60 Hz
5.0682 RMS VA/lb
@Magnetic Field 1.90 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
Electrical Resistivity 0.0000500 ohm-cm0.0000500 ohm-cm
 
Magnetic PropertiesMetricEnglishComments
Core Loss  0.00328 W/kg
@Magnetic Field 0.100 T,
Frequency 50 Hz
0.00149 W/lb
@Magnetic Field 0.100 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.00441 W/kg
@Magnetic Field 0.100 T,
Frequency 60 Hz
0.00200 W/lb
@Magnetic Field 0.100 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.01246 W/kg
@Magnetic Field 0.200 T,
Frequency 50 Hz
0.005652 W/lb
@Magnetic Field 0.200 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.0168 W/kg
@Magnetic Field 0.200 T,
Frequency 60 Hz
0.00762 W/lb
@Magnetic Field 0.200 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.0274 W/kg
@Magnetic Field 0.300 T,
Frequency 50 Hz
0.0124 W/lb
@Magnetic Field 0.300 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.0370 W/kg
@Magnetic Field 0.300 T,
Frequency 60 Hz
0.0168 W/lb
@Magnetic Field 0.300 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.0479 W/kg
@Magnetic Field 0.400 T,
Frequency 50 Hz
0.0217 W/lb
@Magnetic Field 0.400 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.0647 W/kg
@Magnetic Field 0.400 T,
Frequency 60 Hz
0.0293 W/lb
@Magnetic Field 0.400 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.0738 W/kg
@Magnetic Field 0.500 T,
Frequency 50 Hz
0.0335 W/lb
@Magnetic Field 0.500 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.0996 W/kg
@Magnetic Field 0.500 T,
Frequency 60 Hz
0.0452 W/lb
@Magnetic Field 0.500 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.105 W/kg
@Magnetic Field 0.600 T,
Frequency 50 Hz
0.0476 W/lb
@Magnetic Field 0.600 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.1413 W/kg
@Magnetic Field 0.600 T,
Frequency 60 Hz
0.06409 W/lb
@Magnetic Field 0.600 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.1415 W/kg
@Magnetic Field 0.700 T,
Frequency 50 Hz
0.06418 W/lb
@Magnetic Field 0.700 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.1837 W/kg
@Magnetic Field 0.800 T,
Frequency 50 Hz
0.08332 W/lb
@Magnetic Field 0.800 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.190 W/kg
@Magnetic Field 0.700 T,
Frequency 60 Hz
0.0862 W/lb
@Magnetic Field 0.700 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.231 W/kg
@Magnetic Field 0.900 T,
Frequency 50 Hz
0.105 W/lb
@Magnetic Field 0.900 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.246 W/kg
@Magnetic Field 0.800 T,
Frequency 60 Hz
0.112 W/lb
@Magnetic Field 0.800 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.284 W/kg
@Magnetic Field 1.00 T,
Frequency 50 Hz
0.129 W/lb
@Magnetic Field 1.00 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.309 W/kg
@Magnetic Field 0.900 T,
Frequency 60 Hz
0.140 W/lb
@Magnetic Field 0.900 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.344 W/kg
@Magnetic Field 1.10 T,
Frequency 50 Hz
0.156 W/lb
@Magnetic Field 1.10 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.380 W/kg
@Magnetic Field 1.00 T,
Frequency 60 Hz
0.172 W/lb
@Magnetic Field 1.00 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.410 W/kg
@Magnetic Field 1.20 T,
Frequency 50 Hz
0.186 W/lb
@Magnetic Field 1.20 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.459 W/kg
@Magnetic Field 1.10 T,
Frequency 60 Hz
0.208 W/lb
@Magnetic Field 1.10 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.483 W/kg
@Magnetic Field 1.30 T,
Frequency 50 Hz
0.219 W/lb
@Magnetic Field 1.30 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.547 W/kg
@Magnetic Field 1.20 T,
Frequency 60 Hz
0.248 W/lb
@Magnetic Field 1.20 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.562 W/kg
@Magnetic Field 1.40 T,
Frequency 50 Hz
0.255 W/lb
@Magnetic Field 1.40 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.644 W/kg
@Magnetic Field 1.30 T,
Frequency 60 Hz
0.292 W/lb
@Magnetic Field 1.30 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.649 W/kg
@Magnetic Field 1.50 T,
Frequency 50 Hz
0.294 W/lb
@Magnetic Field 1.50 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.650 W/kg
@Magnetic Field 1.50 T,
Frequency 50 Hz
0.295 W/lb
@Magnetic Field 1.50 T,
Frequency 50 Hz
Typical
 0.748 W/kg
@Magnetic Field 1.60 T,
Frequency 50 Hz
0.339 W/lb
@Magnetic Field 1.60 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.749 W/kg
@Magnetic Field 1.40 T,
Frequency 60 Hz
0.340 W/lb
@Magnetic Field 1.40 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.860 W/kg
@Magnetic Field 1.50 T,
Frequency 60 Hz
0.390 W/lb
@Magnetic Field 1.50 T,
Frequency 60 Hz
Typical
 0.865 W/kg
@Magnetic Field 1.50 T,
Frequency 60 Hz
0.392 W/lb
@Magnetic Field 1.50 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 0.870 W/kg
@Magnetic Field 1.70 T,
Frequency 50 Hz
0.395 W/lb
@Magnetic Field 1.70 T,
Frequency 50 Hz
Typical
 0.872 W/kg
@Magnetic Field 1.70 T,
Frequency 50 Hz
0.396 W/lb
@Magnetic Field 1.70 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 0.900 W/kg
@Magnetic Field 1.70 T,
Frequency 50 Hz
0.408 W/lb
@Magnetic Field 1.70 T,
Frequency 50 Hz
Maximum
 0.994 W/kg
@Magnetic Field 1.60 T,
Frequency 60 Hz
0.451 W/lb
@Magnetic Field 1.60 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 1.067 W/kg
@Magnetic Field 1.80 T,
Frequency 50 Hz
0.4840 W/lb
@Magnetic Field 1.80 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 1.154 W/kg
@Magnetic Field 1.70 T,
Frequency 60 Hz
0.5234 W/lb
@Magnetic Field 1.70 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 1.16 W/kg
@Magnetic Field 1.70 T,
Frequency 60 Hz
0.526 W/lb
@Magnetic Field 1.70 T,
Frequency 60 Hz
Typical
 1.20 W/kg
@Magnetic Field 1.70 T,
Frequency 60 Hz
0.544 W/lb
@Magnetic Field 1.70 T,
Frequency 60 Hz
Maximum
 1.405 W/kg
@Magnetic Field 1.80 T,
Frequency 60 Hz
0.6373 W/lb
@Magnetic Field 1.80 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 1.44 W/kg
@Magnetic Field 1.90 T,
Frequency 50 Hz
0.653 W/lb
@Magnetic Field 1.90 T,
Frequency 50 Hz
ASTM A804, 0.27 mm
 1.876 W/kg
@Magnetic Field 1.90 T,
Frequency 60 Hz
0.8509 W/lb
@Magnetic Field 1.90 T,
Frequency 60 Hz
ASTM A804, 0.27 mm
 
Descriptive Properties
Approximate Equivalent International GradeM090-27P5
Magnetostriction 10^8-22ASTM A876, 1.4T, 60Hz, 0.27 mm
 -25ASTM A876, 1.5T, 60Hz, 0.27 mm
 -26ASTM A876, 1.6T, 60Hz, 0.27 mm
 -28ASTM A876, 1.7T, 60Hz, 0.27 mm
Maximum Induction at 800 A/m (T)1.88
Minimum Lamination Factor (%)95
Typical Induction at 800 A/m (T)1.918
Typical Lamination Factor (%)97

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AK Steel DI-MAX® HF-10 Nonoriented Electrical Steel (Extended Electrical/Magnetic Data)
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel
AK Steel TRAN-COR® H-1 CARLITE® Grain Oriented Electrical Steel
AK Steel DI-MAX® M-15 Nonoriented Electrical Steel
AK Steel DI-MAX® HF-10 Nonoriented Electrical Steel

NAKS167 / 140763

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.