MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
GEHR Plastics PA 6 C Nylon 6 Cast
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: Very stressed-relieved and high-molecular weight PA6.

Temperature resistant from -40° to approx. 100°C and high stiffness, hardness and toughness. The good mechanical characteristics will be achieved only after conditioning, this material must be conditioned again after annealing.

Properties:

  • High strength and stiffness
  • High impact and notching impact strength
  • High heat deflection temperature
  • Good at dampening
  • Good glide and emergency operating features
  • Good chemical stability against organic solvents and fuels
  • Size alteration by humidity absorption must be considered
  • Dimension stability, electrical and mechanical properties may become affected by humidity absorption
Applications: Bearing parts (good sliding properties), gear wheels, pump parts, sliding rails, castors (reduction of the noise level), fittings

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccISO 1183
Moisture Absorption at Equilibrium 2.2 %ISO 62
Water Absorption at Saturation 6.5 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 83ISO 868
Ball Indentation Hardness 165 MPaISO 2039
Tensile Strength, Yield 83.0 MPaISO 527
Elongation at Break >= 50 %ISO 527
Modulus of Elasticity 3.47 GPaISO 527
Flexural Strength >= 100 MPaISO 178
Charpy Impact Unnotched NBISO 179
Charpy Impact, Notched 4.00 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohmIEC 60093
Dielectric Constant 3.7
@Frequency 1e+6 Hz
IEC 60250
Dielectric Loss Index 0.030
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 120 µm/m-°CISO 11359
Thermal Conductivity 0.230 W/m-K
@Temperature 20.0 °C
ISO 22007-4
Melting Point 220 °CDIN EN ISO 3146
Maximum Service Temperature, Air 105 °CUL 746B
Minimum Service Temperature, Air -40.0 °CUL 746B
Glass Transition Temp, Tg 40.0 °CDIN EN ISO 3146
Flammability, UL94 HBtest results without UL registration; UL 94
 
Compliance PropertiesOriginal ValueComments
FDA YesPhysiological indifference
 
Descriptive Properties
Bondabilityyes
Colornatural
Physiological indifferenceyes, EEC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Cast
Ensinger Tecast™ 6PA Natural Unfilled Cast Nylon 6 (PA6)
Overview of materials for Nylon 6, Unreinforced
GEHR Plastics ABS Acrylonitrile Butadiene Styrene
EPICHEM PA 6 Polyamide 6

PGEHR016a / 150418

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.