MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

GEHR Plastics ABS Acrylonitrile Butadiene Styrene
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Acrylonitrile Butadiene Styrene copolymer has a good thermal and dimensional stability and scratch resistance.

Advantages

  • good mechanical strength
  • resists scratching
  • high surface strength
  • high impact strength
  • low Moisture absorption
  • high dimensional stability
  • not weather resistant
  • limited resistance to alkalines and acids
Applications
  • Food industry
  • Refrigeration industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccISO 1183
Moisture Absorption at Equilibrium 0.10 %0.10 %ISO 62
Water Absorption at Saturation 0.40 %0.40 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ISO 2039
Hardness, Shore D 7070ISO 868
Ball Indentation Hardness 73.0 MPa10600 psiISO 2039
Tensile Strength at Break 33.0 MPa4790 psiISO 527
Tensile Strength, Yield 37.0 MPa5370 psiISO 527
Elongation at Break 8.0 %8.0 %ISO 527
Elongation at Yield 7.0 %7.0 %ISO 527
Modulus of Elasticity 2.21 GPa321 ksiISO 527
Flexural Strength 67.0 MPa9720 psiISO 178
Charpy Impact Unnotched 33.3 J/cm²158 ft-lb/in²ISO 179
Charpy Impact, Notched 3.70 J/cm²17.6 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FISO 11359
Melting Point 145 °C293 °FDIN EN ISO 3146
Maximum Service Temperature, Air 70.0 °C158 °FUL 746B
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C190 °FISO 75
Vicat Softening Point 103 °C217 °FVST/B/50; ISO 306
Minimum Service Temperature, Air -50.0 °C-58.0 °FUL 746B
Glass Transition Temp, Tg 145 °C293 °FDIN EN ISO 3146
Flammability, UL94 HBHBUL 94
Oxygen Index 20 %20 %ASTM D2863
 
Compliance PropertiesMetricEnglishComments
FDA YesYesPhysiological indifference
 
Descriptive Properties
Acid Resistanceyes
Aromatic Resistanceno
Bondabilityyes
CKW Resistanceno
Colornatural
Hydrocarbonate Resistancelimited
Hydroxide Resistanceno
Ketone Resistancelimited
Physiological indifferenceno, EEC
Resistance Against Hot Waterlimited
UV Stabilizationno

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CENTROPLAST CENTROSOL Acrylonitrile butadiene Styrene copolymer
Elix Polymers ELIX™ 152 I Acrylonitrile Butadiene Styrene (ABS)
Aclo Accucomp ABS ABS801V Automotive Approved Grade
Covestro Bayblend® T65 XF Polycarbonate + ABS
Covestro Bayblend® T85 XF Polycarbonate + ABS

PGEHR012 / 79849

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.