MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 6, Cast
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.11 - 1.17 g/cc0.0401 - 0.0423 lb/in³Average value: 1.15 g/cc Grade Count:65
Water Absorption 0.200 - 7.00 %0.200 - 7.00 %Average value: 0.982 % Grade Count:27
Moisture Absorption at Equilibrium 1.00 - 3.00 %1.00 - 3.00 %Average value: 2.05 % Grade Count:31
Water Absorption at Saturation 2.20 - 7.00 %2.20 - 7.00 %Average value: 5.69 % Grade Count:46
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 82.0 - 88.082.0 - 88.0Average value: 85.8 Grade Count:12
Hardness, Rockwell R 100 - 120100 - 120Average value: 113 Grade Count:19
Hardness, Shore D 75.0 - 85.075.0 - 85.0Average value: 80.5 Grade Count:26
Ball Indentation Hardness 70.0 - 175 MPa10200 - 25400 psiAverage value: 140 MPa Grade Count:37
Tensile Strength, Ultimate 50.0 - 90.0 MPa7250 - 13100 psiAverage value: 75.8 MPa Grade Count:40
Tensile Strength, Yield 40.0 - 100 MPa5800 - 14500 psiAverage value: 71.2 MPa Grade Count:31
Elongation at Break 5.00 - 120 %5.00 - 120 %Average value: 41.1 % Grade Count:47
Elongation at Yield 4.00 - 14.0 %4.00 - 14.0 %Average value: 5.75 % Grade Count:8
Creep Strength 6.00 - 24.0 MPa870 - 3480 psiAverage value: 15.6 MPa Grade Count:15
Modulus of Elasticity 1.30 - 4.20 GPa189 - 609 ksiAverage value: 2.96 GPa Grade Count:62
 0.400 - 0.800 GPa
@Temperature 100 - 100 °C
58.0 - 116 ksi
@Temperature 212 - 212 °F
Average value: 0.600 GPa Grade Count:2
Flexural Yield Strength 20.0 - 150 MPa2900 - 21800 psiAverage value: 95.7 MPa Grade Count:47
Flexural Modulus 1.30 - 3.70 GPa189 - 537 ksiAverage value: 2.76 GPa Grade Count:40
Compressive Yield Strength 6.00 - 162 MPa870 - 23500 psiAverage value: 61.1 MPa Grade Count:41
Compressive Modulus 1.80 - 2.90 GPa261 - 421 ksiAverage value: 2.33 GPa Grade Count:20
Shear Strength 44.8 - 76.0 MPa6500 - 11000 psiAverage value: 66.8 MPa Grade Count:15
Izod Impact, Notched 0.320 - 0.961 J/cm0.600 - 1.80 ft-lb/inAverage value: 0.544 J/cm Grade Count:18
Izod Impact, Notched (ISO) 2.50 - 100000 kJ/m²1.19 - 47600 ft-lb/in²Average value: 11.1 kJ/m² Grade Count:19
Charpy Impact Unnotched 5.00 J/cm² - NB23.8 ft-lb/in² - NBAverage value: 5.00 J/cm² Grade Count:17
Charpy Impact, Notched 0.300 - 10.0 J/cm²1.43 - 47.6 ft-lb/in²Average value: 1.23 J/cm² Grade Count:26
Tensile Impact Strength 72.0 kJ/m²34.3 ft-lb/in²Average value: 72.0 kJ/m² Grade Count:3
Coefficient of Friction 0.0400 - 0.4300.0400 - 0.430Average value: 0.221 Grade Count:43
Coefficient of Friction, Static 0.200 - 0.3500.200 - 0.350Average value: 0.240 Grade Count:5
Tear Strength Test 0.150 - 1.800.150 - 1.80Average value: 0.375 Grade Count:14
K (wear) Factor 8.06 - 500 x 10-8 mm³/N-M4.00 - 248 x 10-10 in³-min/ft-lb-hrAverage value: 219 x 10-8 mm³/N-M Grade Count:9
Limiting Pressure Velocity 0.560 - 1.33 MPa-m/sec16000 - 38000 psi-ft/minAverage value: 0.945 MPa-m/sec Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 - 1.00e+15 ohm-cm1.00e+12 - 1.00e+15 ohm-cmAverage value: 4.06e+14 ohm-cm Grade Count:37
Surface Resistance 1.00e+10 - 1.00e+14 ohm1.00e+10 - 1.00e+14 ohmAverage value: 1.82e+13 ohm Grade Count:37
Dielectric Constant 3.10 - 12.03.10 - 12.0Average value: 3.96 Grade Count:47
Dielectric Strength 15.0 - 100 kV/mm381 - 2540 kV/inAverage value: 28.5 kV/mm Grade Count:49
Dissipation Factor 0.00200 - 0.1500.00200 - 0.150Average value: 0.0283 Grade Count:11
Dielectric Loss Index 0.0120 - 0.1400.0120 - 0.140Average value: 0.0318 Grade Count:17
Comparative Tracking Index 600 V600 VAverage value: 600 V Grade Count:7
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 - 180 µm/m-°C35.0 - 100 µin/in-°FAverage value: 85.9 µm/m-°C Grade Count:66
Specific Heat Capacity 0.290 - 1.70 J/g-°C0.0693 - 0.406 BTU/lb-°FAverage value: 1.55 J/g-°C Grade Count:23
Thermal Conductivity 0.230 - 0.380 W/m-K1.60 - 2.64 BTU-in/hr-ft²-°FAverage value: 0.271 W/m-K Grade Count:45
Melting Point 190 - 238 °C374 - 460 °FAverage value: 220 °C Grade Count:63
Maximum Service Temperature, Air 60.0 - 180 °C140 - 356 °FAverage value: 131 °C Grade Count:64
Deflection Temperature at 0.46 MPa (66 psi) 160 - 221 °C320 - 430 °FAverage value: 203 °C Grade Count:30
Deflection Temperature at 1.8 MPa (264 psi) 80.0 - 204 °C176 - 399 °FAverage value: 120 °C Grade Count:40
Minimum Service Temperature, Air -100 - -20.0 °C-148 - -4.00 °FAverage value: -43.3 °C Grade Count:41
Glass Transition Temp, Tg 5.00 - 50.0 °C41.0 - 122 °FAverage value: 40.5 °C Grade Count:9
Flammability, UL94 HB - V-2HB - V-2Grade Count:30
Oxygen Index 25.0 %25.0 %Average value: 25.0 % Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Nylon 6, Extruded
DuPont Mobility and Materials Vespel® SP-1 Polyimide, Direct formed
Overview of materials for Nylon 66, Unreinforced

O2402 / 77963

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.