MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lubrizol Advanced Materials Pearlthane® 12C75 Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Pearlthane® 12C75 is a standard polyester based TPU supplied in form of translucent, colorless pellets, specially designed for compounds in which TPU is used as an additive. Features include low softness without plasticizer and a low melting point. Pearlthane® 12C75 is intended for compounding applications of a variety engineering plastic.

Information provided by Merquinsa.

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 21.6 kg,
Temperature 125 - 135 °C
10 g/10 min
@Load 47.6 lb,
Temperature 257 - 275 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7878ASTM D2240
Tensile Strength, Yield 20.03 MPa2905 psiASTM D412
Elongation at Break 745 %745 %ASTM D412
100% Modulus 4.01 MPa
@Strain 100 %
581 psi
@Strain 100 %
ASTM D412
300% Modulus 5.52 MPa
@Strain 300 %
800 psi
@Strain 300 %
ASTM D412
Tear Strength 70.1 kN/m400 pliASTM D624 DIE C
Abrasion 2525[mm^3]; ISO 4649
 
Thermal PropertiesMetricEnglishComments
Melting Point 125 - 135 °C257 - 275 °FMQSA 111
Glass Transition Temp, Tg -35.6 °C-32.0 °FDSC, 50°F/min; ISO 11357-2
 
Processing PropertiesMetricEnglishComments
Zone 1 120 - 130 °C248 - 266 °F
Zone 2 130 - 140 °C266 - 284 °F
Zone 3 140 - 150 °C284 - 302 °F
Zone 4 145 - 155 °C293 - 311 °F
Die Temperature 145 - 155 °C293 - 311 °F
Moisture Content <= 0.10 %<= 0.10 %MQSA 44
Screw Speed 50 rpm50 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU
Lubrizol Advanced Materials PEARLTHANE® 11T60D Thermoplastic Polyurethane Elastomer

PMES80A / 159336

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.