MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Type : Pearlthane® 11T85 is a polycaprolactone copolyester-based thermoplastic polyurethane.

Main Application : Injection Moulding

Special Features : Adequate hardness, excellent mechanical properties and easy processing.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8686ISO 868
Tensile Strength, Ultimate 40.0 MPa5800 psiISO 527-2/5A/500
Elongation at Break 640 %640 %ISO 527-2/5A/500
50% Modulus 5.00 MPa
@Strain 50 %
5.00 MPa
@Strain 50 %
ISO 527-2/5A/500
100% Modulus 6.00 MPa
@Strain 100 %
870 psi
@Strain 100 %
ISO 527-2/5A/500
300% Modulus 10.0 MPa
@Strain 300 %
1450 psi
@Strain 300 %
ISO 527-2/5A/500
Tear Strength 90.0 kN/m514 pliISO 34-1B
Abrasion 2020mm3; ISO 4649-a
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 87.0 °C189 °FISO 306
 
Processing PropertiesMetricEnglishComments
Feed Temperature 40.0 °C104 °F
Nozzle Temperature 210 °C410 °F
Zone 1 195 °C383 °F
Zone 2 200 °C392 °F
Zone 3 210 °C410 °F
Zone 4 210 °C410 °F
Dry Time 3.00 hour
@Temperature 100 °C
3.00 hour
@Temperature 212 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether
Celanese Celstran® TPU-GF30-01-US TPU, 30% Glass Reinforced
3D Systems DuraForm® HST Fiber Filled Nylon for SLS Systems
BASF Ultramid® 8202 PA6 (Dry)

PMER22 / 52823

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.