MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Type: Pearlthane® 11H98 is a polycaprolactone copolyester-based thermoplastic polyurethane.

Main Application : Extrusion/Moulding

Special Features : Combining a unique set of properties such as mechanical properties, chemical resistance and processability for very demanding applications.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9898ISO 868
Hardness, Shore D 5252ISO 868
Tensile Strength, Yield 35.06 MPa5085 psiISO 527-2/5A/500
Elongation at Break 600 %600 %ISO 527-2/5A/500
50% Modulus 10.0 MPa
@Strain 50 %
10.0 MPa
@Strain 50 %
ISO 527-2/5A/500
100% Modulus 11.00 MPa
@Strain 100 %
1595 psi
@Strain 100 %
ISO 527-2/5A/500
300% Modulus 19.0 MPa
@Strain 300 %
2760 psi
@Strain 300 %
ISO 527-2/5A/500
Tear Strength 150 kN/m855 pliUnnicked; ISO 34-1B
Abrasion 2525loss (mm³); ISO 4649-A
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 124 °C255 °FISO 306
 
Processing PropertiesMetricEnglishComments
Zone 1 200 - 210 °C392 - 410 °F
Zone 2 205 - 215 °C401 - 419 °F
Zone 3 215 - 225 °C419 - 437 °F
Zone 4 220 - 230 °C428 - 446 °F
Adapter Temperature 200 - 230 °C392 - 446 °F5
Die Temperature 225 - 235 °C437 - 455 °F6
 225 - 235 °C437 - 455 °FTIP, 7
Dry Time 3.00 hour
@Temperature 100 °C
3.00 hour
@Temperature 212 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 11T60D Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU
Lubrizol Advanced Materials Pearlthane® Clear 15N70 Polyether based TPU

PMES52 / 88429

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.