MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: PEARLTHANE® 15N95UV is a polyether copolymer-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resistance. It can be extruded and injection-molded. PEARLTHANE® 15N95UV can be used for high performance animal ear tags and a variety of technical parts for outdoor use. When extruded, it can be used for tubing and profiles. To improve the microbiological protection of PEARLTHANE® 15N95UV, it is necessary to add a biocide, preferably in form of TPU-based masterbatch.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595ISO 868
Hardness, Shore D 4545ISO 868
Tensile Strength, Yield 35.00 MPa5076 psiISO 527-2/5A/500
Elongation at Break 545 %545 %ISO 527-2/5A/500
50% Modulus 10.0 MPa
@Strain 50 %
10.0 MPa
@Strain 50 %
ISO 527-2/5A/500
100% Modulus 11.0 MPa
@Strain 100 %
1600 psi
@Strain 100 %
ISO 527-2/5A/500
300% Modulus 19.00 MPa
@Strain 300 %
2755 psi
@Strain 300 %
ISO 527-2/5A/500
Tear Strength 145 kN/m830 pliISO 34-1B
Abrasion 2525Resistance (mm³); ISO 4649-A
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 119 °C246 °FISO 306 (A50)
 
Processing PropertiesMetricEnglishComments
Zone 1 200 °C392 °F
Zone 2 230 °C446 °F
Zone 3 230 °C446 °F
Zone 4 220 °C428 °F
Adapter Temperature 195 °C383 °F(5)
Die Temperature 195 °C383 °F(6)
 195 °C383 °FTIP (7)
Drying Temperature 100 °C
@Time 10800 - 14400 sec
212 °F
@Time 3.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 11T60D Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU
Lubrizol Advanced Materials Pearlthane® Clear 15N70 Polyether based TPU

PMES46 / 88423

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.