MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environments. Not only does it have excellent holding power, but also its adhesion strength is significantly higher than typical pressure sensitive tapes. 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082UV and 9085UV have a UV fluoresce agent to allow black light inspection during converting and assembly. These adhesive transfer tapes are ideal for use in many industrial applications subjected to higher temperature environments. Typical examples are for automotive under-hood applications that require both higher processing and operating temperatures. Other areas include printed circuit boards and heat sink bonding in many electronics applications subjected to high solder reflow temperatures.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³
Thickness 50.8 microns2.00 milAdhesive
 81.3 microns3.20 milRelease Liner
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  0.0700 MPa
@Temperature 175 °C
10.2 psi
@Temperature 347 °F
T-Block on Aluminum; ASTM D987
 0.0700 MPa
@Temperature 230 °C
10.2 psi
@Temperature 446 °F
T-Block on Aluminum; ASTM D987
 0.100 MPa
@Temperature 107 °C
14.5 psi
@Temperature 225 °F
T-Block on Aluminum; ASTM D987
 0.100 MPa
@Temperature 150 °C
14.5 psi
@Temperature 302 °F
T-Block on Aluminum; ASTM D987
 0.345 MPa
@Temperature 23.0 °C
50.0 psi
@Temperature 73.4 °F
T-Block on Aluminum; ASTM D987
Shear Strength  0.103 MPa
@Temperature 230 °C
15.0 psi
@Temperature 446 °F
Over-Lap Shear on Stainless Steel; ASTM D1002
 0.138 MPa
@Temperature 175 °C
20.0 psi
@Temperature 347 °F
Over-Lap Shear on Stainless Steel; ASTM D1002
 0.207 MPa
@Temperature 150 °C
30.0 psi
@Temperature 302 °F
Over-Lap Shear on Stainless Steel; ASTM D1002
 0.241 MPa
@Temperature 107 °C
35.0 psi
@Temperature 225 °F
Over-Lap Shear on Stainless Steel; ASTM D1002
 0.621 MPa
@Temperature 23.0 °C
90.0 psi
@Temperature 73.4 °F
Over-Lap Shear on Stainless Steel; ASTM D1002
Peel Strength  0.263 kN/m
@Temperature 230 °C
1.50 pli
@Temperature 446 °F
Adhesion on Aluminum; ASTM D3330
 0.526 kN/m
@Temperature 175 °C
3.00 pli
@Temperature 347 °F
Adhesion on Aluminum; ASTM D3330
 0.614 kN/m
@Temperature 150 °C
3.50 pli
@Temperature 302 °F
Adhesion on Aluminum; ASTM D3330
 0.701 kN/m
@Temperature 107 °C
4.00 pli
@Temperature 225 °F
Adhesion on Aluminum; ASTM D3330
 0.877 kN/m
@Temperature 23.0 °C
5.00 pli
@Temperature 73.4 °F
Adhesion on Aluminum; ASTM D3330
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance >= 1.00e+6 ohm>= 1.00e+6 ohmASTM D1000
Dielectric Strength  11.8 kV/mm
@Temperature 23.0 °C
300 kV/in
@Temperature 73.4 °F
ASTM D149-97A
 30.3 kV/mm
@Temperature 175 °C
770 kV/in
@Temperature 347 °F
ASTM D149-97A
 34.3 kV/mm
@Temperature 150 °C
870 kV/in
@Temperature 302 °F
ASTM D149-97A
 47.2 kV/mm
@Temperature 23.0 °C
1200 kV/in
@Temperature 73.4 °F
ASTM D149-97A
 
Thermal PropertiesMetricEnglishComments
CTE, linear 77.0 µm/m-°C42.8 µin/in-°F
Thermal Conductivity 0.669 W/m-K4.64 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 177 °C351 °FLong term
 280 °C536 °FShort term
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Adhesive TypeAcrylic Adhesive
AppearanceClear
LinerWhite printed paper

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M F-9465PC Adhesive Transfer Tape
3M 9471FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9447 Adhesive Transfer Tape
3M 9437 Adhesive Transfer Tape with Adhesive 100MP

PMM33332 / 168079

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.