MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 9447 Adhesive Transfer Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ Adhesive Transfer Tape 9447 is specifically designed for use with 3M™ Label Component Systems for protected graphics printing of polyester films. Also can be used in constructing custom tamper-indicating labels.

Features:

  • 3M™ Adhesive 320 is used for general purpose applications and offers excellent flagging resistance and adhesion to a variety of substrates.
  • The liner provides an ideal surface for rotary die-cutting.
  • Adhesive has a temperature range of -40°F (-40°C) to 150°F (65°C) for days or weeks and to 250°F (121°C) for minutes or hours.
Applications:
  • Used to make tamper-indicating labels with Label Component System films and solutions. These labels may be used as seals for over-the-counter drugs, banking envelopes, non-transferable automobile inspection labels and a variety of other applications.
  • A component in the construction of labels with protected, or sub-surface printed graphics, used in harsh environments such as automotive under hood or outdoor environments.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 25.4 microns1.00 milAdhesive
 81.3 microns3.20 milLiner
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.09861 kN/m0.5625 pliPolypropylene, 90° peel, 12"/min, 72 hr dwell RT; ASTM D3330
 0.307 kN/m1.75 pliStainless Steel, 90° peel, 12"/min, 20 min dwell; ASTM D3330
 0.3725 kN/m2.125 pliStainless Steel, 90° peel, 12"/min, 72 hr dwell RT; ASTM D3330
 0.38347 kN/m2.1875 pliPolycarbonate, 90° peel, 12"/min, 72 hr dwell RT; ASTM D3330
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Liner55# Densified Kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M ScotchCal™ 3690E Graphic Film Material
3M F-9465PC Adhesive Transfer Tape
3M 9471FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9437 Adhesive Transfer Tape with Adhesive 100MP

PMM33216 / 167963

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.