MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
Categories: Polymer; Adhesive

Material Notes: Features:
  • Clear Polyester (PET)
  • Quick flowing acrylic adhesive speeds lamination process
  • Excellent initial adhesion, especially to LSE (low surface energy) plastics
  • Bonds graphics to powder coatings, LSE plastics and oily metals
  • Use on textured plastics, fabrics and coated papers
  • Moisture-stable liner is rotary die-cutable

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milLiner
 88.9 microns3.50 milAdhesive
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.877 kN/m5.00 pliABS, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330
 0.97511 kN/m5.5625 pliPolypropylene, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330
 0.9861 kN/m5.625 pliStainless Steel, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330
 1.10 kN/m6.25 pliStainless Steel, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
 1.1285 kN/m6.4375 pliPolypropylene, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
 1.2381 kN/m7.0625 pliABS, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °FLong term
 148 °C298 °FShort term
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 463 Adhesive Transfer Tape with 3M Adhesive 400
3M 9471FL Adhesive Transfer Tape with 300LSE Adhesive
3M F-9465PC Adhesive Transfer Tape
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M 941 Adhesive Transfer Tapes with Adhesive 100

PMM33217 / 167964

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.