MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 463 Adhesive Transfer Tape with 3M Adhesive 400
Categories: Polymer; Adhesive

Material Notes: 3M™ Adhesive Transfer Tapes 463, 465, 9457 and 9665 with 3M™ Adhesive 400 are ideal for bonding together a wide variety of similar and dissimilar materials such as metals, glass, wood, papers, paints, and many plastics.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milTape Only
 102 microns4.00 milRelease Liner
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.27391 kN/m1.5625 plito Steel; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.0 °C180 °FLong term
 121 °C250 °FShort term
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Adhesive CarrierNone
Adhesive Type400
Liner60# Unbleached Densified Kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
3M 927 Adhesive Transfer Tapes with Adhesive 300
3M 9471FL Adhesive Transfer Tape with 300LSE Adhesive
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M 9445 Adhesive Transfer Tapes with Adhesive 350

PMM33172 / 167919

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.