MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
Categories: Polymer; Adhesive

Material Notes: 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as a result of 3M’s innovative, proprietary process, 3M™ Adhesive 200MP also offers the following excellent performance characteristics. Clarity (virtually free of vapor inclusions that are commonly found in adhesives produced by the traditional solvent coating technique). Excellent high temperature performance as well as excellent shear strength (that minimizes edge lifting and slippage of parts). Excellent resistance to harsh environments; this adhesive can withstand splashes of organic solvents, weak acids and bases and salt water, cleaning solutions, germicidals, disinfectants, oils, etc. In addition, it performs well after exposure to humidity and hot/cold cycles. Provides some initial repositionability when bonding to plastic parts (not metal) which allows graphic parts to be lifted and repositioned if initial alignment is incorrect. Finally, this adhesive family is provided with a variety of liner configurations to help ensure excellent process flexibility.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 132 microns5.20 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 0.352 MPa51.1 psiASTM D2370-82
Elongation at Break 1915 %
@Thickness 0.127 mm
1915 %
@Thickness 0.00500 in
ASTM D2370-82
Adhesive Bond Strength 0.752 MPa
@Thickness 0.127 mm
109 psi
@Thickness 0.00500 in
Tensile Lap Shear – Peak Stress; ASTM D1002-72
Peel Strength 0.51494 kN/m2.9375 plito Stainless Steel, 90° peel, 2 mil aluminum foil backing, 15 minute room temperature
 0.570 kN/m3.25 pli72 hour RT rigid PVC (unplasticized), 90° peel, 2 mil aluminum foil backing
 0.6355 kN/m3.625 pli72 hour RT polycarbonate, 90° peel, 2 mil aluminum foil backing
 0.66833 kN/m3.8125 pli72 hour RT acrylic, 90° peel, 2 mil aluminum foil backing
 0.6793 kN/m3.875 pli72 hour RT ABS, 90° peel, 2 mil aluminum foil backing
 0.71216 kN/m4.0625 pli72 hour RT polycarbonate, 90° peel, 5 mil aluminum foil backing
 0.7231 kN/m4.125 plito Stainless Steel, 90° peel, 5 mil aluminum foil backing, 15 minute room temperature
 0.73407 kN/m4.1875 pli72 hour RT acrylic, 90° peel, 5 mil aluminum foil backing
 0.745 kN/m4.25 pli72 hour RT ABS, 90° peel, 5 mil aluminum foil backing
 0.75598 kN/m4.3125 pli72 hour RT rigid PVC (unplasticized), 90° peel, 5 mil aluminum foil backing
 0.84363 kN/m4.8125 plito Stainless Steel, 72 hour RT - 180° peel, 2 mil al foil
 0.84363 kN/m4.8125 pli72 hour RT aluminum, 90° peel, 2 mil aluminum foil backing
 0.877 kN/m5.00 pli72 hour RT glass, 90° peel, 2 mil aluminum foil backing
 0.8984 kN/m5.125 plito Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour RT
 1.01 kN/m5.75 pli72 hour RT glass, 90° peel, 5 mil aluminum foil backing
 1.2600 kN/m7.1875 pli72 hour RT aluminum, 90° peel, 5 mil aluminum foil backing
 1.293 kN/m7.375 plito Stainless Steel, 90° peel, 5 mil aluminum foil backing, 72 hour RT
 1.4572 kN/m8.3125 plito Stainless Steel, 72 hour RT - 180° peel, 5 mil al foil
 1.84 kN/m10.5 plito Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour 158°F (70°C)
 1.983 kN/m11.31 plito Stainless Steel, 90° peel, 5 mil aluminum foil backing, 72 hour 158°F (70°C)
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength  23.6 kV/mm
@Thickness 0.127 mm
600 kV/in
@Thickness 0.00500 in
ASTM D149-92
 34.6 kV/mm
@Thickness 0.0508 mm
880 kV/in
@Thickness 0.00200 in
500 vac, rms [60 hz/sec]; ASTM D149-92
Dielectric Breakdown  1760 V
@Thickness 0.0508 mm,
Frequency 1000 Hz
1760 V
@Thickness 0.00200 in,
Frequency 1000 Hz
ASTM D 150-92
 3000 V
@Thickness 0.127 mm,
Frequency 1000 Hz
3000 V
@Thickness 0.00500 in,
Frequency 1000 Hz
ASTM D 150-92
Dissipation Factor  0.021
@Thickness 0.0508 mm
0.021
@Thickness 0.00200 in
 0.022
@Thickness 0.127 mm
0.022
@Thickness 0.00500 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear  -6.00 µm/m-°C
@Thickness 0.0508 mm
-3.33 µin/in-°F
@Thickness 0.00200 in
first heat; ASTM D 696
 28.0 µm/m-°C
@Thickness 0.0508 mm
15.6 µin/in-°F
@Thickness 0.00200 in
first heat; ASTM D 696
 72.0 µm/m-°C
@Thickness 0.127 mm
40.0 µin/in-°F
@Thickness 0.00500 in
second heat; ASTM D 696
 92.0 µm/m-°C
@Thickness 0.127 mm
51.1 µin/in-°F
@Thickness 0.00500 in
second heat; ASTM D 696
Thermal Conductivity  0.170 W/m-K
@Thickness 0.0508 mm
1.18 BTU-in/hr-ft²-°F
@Thickness 0.00200 in
 0.180 W/m-K
@Thickness 0.127 mm
1.25 BTU-in/hr-ft²-°F
@Thickness 0.00500 in
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
AppearanceClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 9086 High Performance Double Coated Tapes with Adhesive 375
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9471FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9471 Adhesive Transfer Tapes with Adhesive 300
3M 9462P Adhesive Transfer Tapes with Adhesive 100

PMM33175 / 167922

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.