MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M 9437 Adhesive Transfer Tape with Adhesive 100MP
Categories: Polymer; Adhesive

Material Notes: 3M™ Adhesive Transfer Tape 9437 with 3M™ Adhesive 100MP is designed for harsh environments such as automotive, aerospace and outdoor applications.

Features:

  • Excellent temperature and chemical resistance.
  • Exceptional shear holding strength at elevated temperatures.
  • Strong bond to metals and high surface energy plastics (e.g. ABS, polycarbonate).
  • Polyester liner provides excellent die-cutting surface

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 mil
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.18626 kN/m1.0625 pliPolypropylene, 72 Hour Dwell, (90° peel, 12"/min.) on 2 mil aluminum; ASTM D3330
 0.51494 kN/m2.9375 pliPolycarbonate, 72 Hour Dwell, (90° peel, 12"/min.) on 2 mil aluminum; ASTM D3330
 0.526 kN/m3.00 pliStainless Steel, 20 Minute Dwell, (90° peel, 12"/min.) on 2 mil aluminum; ASTM D3330
 0.79981 kN/m4.5625 pliStainless Steel, 72 Hour Dwell, (90° peel, 12"/min.) on 2 mil aluminum; ASTM D3330
 1.3695 kN/m7.8125 pliStainless Steel, Ultimate Bond, (90° peel, 12"/min.) on 2 mil aluminum; ASTM D3330
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Adhesive Type100MP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M F-9465PC Adhesive Transfer Tape
3M 9471FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9447 Adhesive Transfer Tape
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape

PMM33209 / 167956

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.