MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Butene-1 Combustible gas
Categories: Fluid

Material Notes: CAS No: 106-98-9

Butene-1 is a colorless, combustible gas with a characteristic odor. It is easily condensable under pressure. Butene-1 is soluble in hydrocarbons, alcohols and ethers, but virtually insoluble in water (0.5 g/l at 20°C). Butene-1 is highly flammable.

Application:

  • comonomer for polyethylene (LLDPE, HDPE)
  • comonomer for ethylene/propylene copolymers
  • alkylation products
Antioxidants, plasticizers, herbicides, corrosion inhibitors or additives to lubricating and hydraulic oils are accessible via the intermediate products sec.-butanol, butane oxide or amyl alcohol.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.01 g/cc
 0.5699 g/cc
@Temperature 40.0 °C
 0.5825 g/cc
@Temperature 30.0 °C
 0.5951 g/cc
@Temperature 20.0 °C
 0.6077 g/cc
@Temperature 10.0 °C
 0.6203 g/cc
@Temperature 0.000 °C
 0.6329 g/cc
@Temperature -10.0 °C
Molecular Weight 56.11 g/mol
Vapor Pressure 0.873 bar
@Temperature -10.0 °C
 1.283 bar
@Temperature 0.000 °C
 1.834 bar
@Temperature 10.0 °C
 2.545 bar
@Temperature 20.0 °C
 3.45 bar
@Temperature 30.0 °C
 4.575 bar
@Temperature 40.0 °C
 5.94 bar
@Temperature 50.0 °C
 7.60 bar
@Temperature 60.0 °C
 11.85 bar
@Temperature 80.0 °C
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 40.2 bar
Critical Temperature 146.4 °C
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.51 J/g-°Cgaseous at 25°C
 2.30 J/g-°Cliquid at boiling point
Boiling Point -6.30 °C
@Pressure 0.1013 MPa
 50.4 °C
@Pressure 0.600 MPa
 
Descriptive Properties
Content<0.05%Butene-2 (cis-+trans-isomers)
 <0.2%Butane (n-and isobutane)
 <0.2%Isobutene
 <0.5 ml/m3Carbon monoxide
 <1 mg/kgAlcohols
 <1 ml/m3Carbon dioxide
 <10 mg/kgWater
 <2 mg/kgCarbonyls
 <30%Butadiene-1,3
 <5 mg/kgAcetylenes (calc. as 1-butyne)
 >1 mg/kgOxygen
 >1 mg/kgSulfur
 >1 mg/kgChlorine
 >99.6%Butene-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Honeywell Solstice® Gas Blowing Agent
Overview of materials for PVC, Foam Grade
Overview of materials for Polyetherimide (PEI)
Honeywell Genetron® AZ-20 Refrigerant

PEVONIL959 / 197163

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.