MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Honeywell Genetron® AZ-20 Refrigerant
Categories: Fluid

Material Notes: Genetron® AZ-20® (an azeotropic mixture of HFC-32/HFC-125, assigned R-410A by ASHRAE), has been developed by Honeywell to serve as a long-term, non-ozone-depleting replacement for HCFC-22 in a variety of new-equipment applications. Genetron AZ-20 has a significantly higher capacity and pressure than HCFC-22 and an intrinsically low toxicity. Because it behaves like an azeotrope, Genetron AZ-20 is easy to service in the field. Genetron AZ-20 is patented and has been recognized by Underwriters’ Laboratory as practically non-flammable.

Applications:
Unitary Air Conditioning: Genetron AZ-20 is the ideal non-ozone-depleting, long-term replacement for HCFC-22 in new residential and light commercial unitary air conditioning systems. In new unitary systems optimized for its use, with either scroll or reciprocating compressors, Genetron AZ-20 has shown in tests to have a 5-to-6 percent higher Energy Efficiency Rating (EER) than HCFC-22. Genetron AZ-20 also has a higher capacity and pressure than HCFC-22, enabling the design of smaller, more compact air-conditioning equipment.
Chillers: Genetron AZ-20 serves as an excellent replacement for HCFC-22 in new chillers, particularly positive displacement chillers. It also may serve as a retrofit fluid for replacing HCFC-22 in some existing chillers with components approved for high pressure, especially those with flooded heat-exchangers. Honeywell recommends contacting the original chiller equipment manufacturer before carrying out any retrofit.
Commercial Refrigeration: Genetron AZ-20 may be used as a replacement for HCFC-22 in new medium-temperature commercial refrigeration systems, including supermarket display cases and reach-in coolers.

Chemical Name: Difluoromethane/ Pentafluoroethane

Molecular Formula : CH2F2/CHF2CF3

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.00417 g/cc0.000150 lb/in³Vapor at Boiling Point
 0.4596 g/cc0.01660 lb/in³Critical
 1.059 g/cc0.03825 lb/in³Liquid
Volatiles 99.99 %99.99 %
Viscosity  12.92 cP
@Temperature 5.00 °C
12.92 cP
@Temperature 41.0 °F
Vapor
 14.5 cP
@Temperature 25.0 °C
14.5 cP
@Temperature 77.0 °F
Vapor
 17.43 cP
@Temperature 50.0 °C
17.43 cP
@Temperature 122 °F
Vapor
 81.8 cP
@Temperature 50.0 °C
81.8 cP
@Temperature 122 °F
Liquid
 116.73 cP
@Temperature 25.0 °C
116.73 cP
@Temperature 77.0 °F
Liquid
 150.87 cP
@Temperature 5.00 °C
150.87 cP
@Temperature 41.0 °F
Liquid
Molecular Weight 72.6 g/mol72.6 g/mol
Vapor Pressure 16.52 bar12390 torr
Surface Tension  0.901 dynes/cm
@Temperature 60.0 °C
0.901 dynes/cm
@Temperature 140 °F
 1.423 dynes/cm
@Temperature 55.0 °C
1.423 dynes/cm
@Temperature 131 °F
 1.987 dynes/cm
@Temperature 50.0 °C
1.987 dynes/cm
@Temperature 122 °F
 2.585 dynes/cm
@Temperature 45.0 °C
2.585 dynes/cm
@Temperature 113 °F
 3.212 dynes/cm
@Temperature 40.0 °C
3.212 dynes/cm
@Temperature 104 °F
 3.864 dynes/cm
@Temperature 35.0 °C
3.864 dynes/cm
@Temperature 95.0 °F
 5.235 dynes/cm
@Temperature 25.0 °C
5.235 dynes/cm
@Temperature 77.0 °F
 5.539 dynes/cm
@Temperature 30.0 °C
5.539 dynes/cm
@Temperature 86.0 °F
 5.949 dynes/cm
@Temperature 20.0 °C
5.949 dynes/cm
@Temperature 68.0 °F
 6.681 dynes/cm
@Temperature 15.0 °C
6.681 dynes/cm
@Temperature 59.0 °F
 7.429 dynes/cm
@Temperature 10.0 °C
7.429 dynes/cm
@Temperature 50.0 °F
 8.192 dynes/cm
@Temperature 5.00 °C
8.192 dynes/cm
@Temperature 41.0 °F
 8.969 dynes/cm
@Temperature 0.000 °C
8.969 dynes/cm
@Temperature 32.0 °F
 9.76 dynes/cm
@Temperature -5.00 °C
9.76 dynes/cm
@Temperature 23.0 °F
 10.564 dynes/cm
@Temperature -10.0 °C
10.564 dynes/cm
@Temperature 14.0 °F
 11.38 dynes/cm
@Temperature -15.0 °C
11.38 dynes/cm
@Temperature 5.00 °F
 12.208 dynes/cm
@Temperature -20.0 °C
12.208 dynes/cm
@Temperature -4.00 °F
 13.046 dynes/cm
@Temperature -25.0 °C
13.046 dynes/cm
@Temperature -13.0 °F
 13.895 dynes/cm
@Temperature -30.0 °C
13.895 dynes/cm
@Temperature -22.0 °F
 14.754 dynes/cm
@Temperature -35.0 °C
14.754 dynes/cm
@Temperature -31.0 °F
 15.622 dynes/cm
@Temperature -40.0 °C
15.622 dynes/cm
@Temperature -40.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 49.02 bar36770 torr
Critical Temperature 71.356 °C160.44 °F
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 2.00 kV/mm
@Pressure 0.101 MPa
50.8 kV/in
@Pressure 14.7 psi
Dielectric Breakdown  9580 V
@Pressure 1.00 MPa,
Temperature 7.22 °C
9580 V
@Pressure 145 psi,
Temperature 45.0 °F
0.02 d (Gap) in
 17000 V
@Pressure 1.647 MPa,
Temperature 25.0 °C
17000 V
@Pressure 238.9 psi,
Temperature 77.0 °F
0.02 d (Gap) in
 28100 V
@Pressure 2.62 MPa,
Temperature 43.3 °C
28100 V
@Pressure 380 psi,
Temperature 110 °F
0.02 d (Gap) in
 55400 V
@Pressure 1.00 MPa,
Temperature 7.22 °C
55400 V
@Pressure 145 psi,
Temperature 45.0 °F
0.01 d (Gap) in
 92500 V
@Pressure 1.647 MPa,
Temperature 25.0 °C
92500 V
@Pressure 238.9 psi,
Temperature 77.0 °F
0.01 d (Gap) in
 148300 V
@Pressure 2.62 MPa,
Temperature 43.3 °C
148300 V
@Pressure 380 psi,
Temperature 110 °F
0.01 d (Gap) in
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 273.35 J/g
@Pressure 0.101 MPa
117.43 BTU/lb
@Pressure 14.7 psi
at Boiling Point
Specific Heat Capacity 1.72 J/g-°C0.410 BTU/lb-°FLiquid
 0.711 J/g-°C
@Pressure 0.101 MPa
0.170 BTU/lb-°F
@Pressure 14.7 psi
Vapor
Thermal Conductivity  0.0128 W/m-K
@Temperature 5.00 °C
0.0888 BTU-in/hr-ft²-°F
@Temperature 41.0 °F
Vapor
 0.0157 W/m-K
@Temperature 25.0 °C
0.109 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
Vapor
 0.0241 W/m-K
@Temperature 50.0 °C
0.167 BTU-in/hr-ft²-°F
@Temperature 122 °F
Vapor
 0.0791 W/m-K
@Temperature 50.0 °C
0.549 BTU-in/hr-ft²-°F
@Temperature 122 °F
Liquid
 0.0924 W/m-K
@Temperature 25.0 °C
0.641 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
Liquid
 0.1034 W/m-K
@Temperature 5.00 °C
0.7176 BTU-in/hr-ft²-°F
@Temperature 41.0 °F
Liquid
Melting Point -155 °C-247 °F
Boiling Point -51.4 °C
@Pressure 0.101 MPa
-60.6 °F
@Pressure 14.7 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Expanded Polystyrene (EPS)
Overview of materials for Polyimide
2-Octanol, C8H18O
2-Butoxyethanol, C6H14O2
2-Butanol (CH3CH2CH(OH)CH3; secondary-Butyl Alcohol)

PHONWL134 / 179679

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.