Physical Properties | Metric | English | Comments |
---|
Density | 0.0500 - 1.90 g/cc | 0.00181 - 0.0686 lb/in³ |
Filler Content | 5.00 - 50.0 % | 5.00 - 50.0 % |
Water Absorption | 0.0150 - 1.30 % | 0.0150 - 1.30 % |
Moisture Absorption at Equilibrium | 0.000 - 1.30 % | 0.000 - 1.30 % |
Water Absorption at Saturation | 0.100 - 2.90 % | 0.100 - 2.90 % |
Additive Loading | 10.0 - 40.0 % | 10.0 - 40.0 % |
Particle Size | 15.0 µm | 15.0 µm |
Viscosity | 3.00 - 87.0 cP @Temperature 220 - 360 °C | 3.00 - 87.0 cP @Temperature 428 - 680 °F |
| 3.00 - 87.0 cP @Load 2.16 - 10.0 kg | 3.00 - 87.0 cP @Load 4.76 - 22.0 lb |
Maximum Moisture Content | 0.0200 | 0.0200 |
Linear Mold Shrinkage | 0.000 - 0.0230 cm/cm | 0.000 - 0.0230 in/in |
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0240 cm/cm | 0.00100 - 0.0240 in/in |
Melt Flow | 1.80 - 113 g/10 min | 1.80 - 113 g/10 min |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Rockwell M | 85.0 - 115 | 85.0 - 115 |
Hardness, Rockwell R | 100 - 127 | 100 - 127 |
Hardness, Shore D | 72.0 - 93.0 | 72.0 - 93.0 |
Ball Indentation Hardness | 125 - 220 MPa | 18100 - 31900 psi |
Tensile Strength, Ultimate | 1.00 - 650 MPa | 145 - 94300 psi |
Tensile Strength, Yield | 20.0 - 255 MPa | 2900 - 37000 psi |
Elongation at Break | 0.500 - 110 % | 0.500 - 110 % |
Elongation at Yield | 0.700 - 400 % | 0.700 - 400 % |
Modulus of Elasticity | 0.00280 - 56.0 GPa | 0.406 - 8120 ksi |
Flexural Yield Strength | 17.9 - 770 MPa | 2600 - 112000 psi |
| 85.0 - 214 MPa @Temperature 80.0 - 200 °C | 12300 - 31000 psi @Temperature 176 - 392 °F |
Flexural Modulus | 0.380 - 46.0 GPa | 55.1 - 6670 ksi |
| 7.30 - 17.9 GPa @Temperature 80.0 - 200 °C | 1060 - 2600 ksi @Temperature 176 - 392 °F |
Flexural Strain at Break | 0.900 - 3.80 % | 0.900 - 3.80 % |
| 1.00 - 2.60 % @Temperature 80.0 - 200 °C | 1.00 - 2.60 % @Temperature 176 - 392 °F |
Compressive Yield Strength | 0.500 - 1130 MPa | 72.5 - 163000 psi |
Compressive Modulus | 0.0220 - 52.0 GPa | 3.19 - 7540 ksi |
Poissons Ratio | 0.300 - 0.440 | 0.300 - 0.440 |
Shear Modulus | 0.0130 - 4.73 GPa | 1.89 - 685 ksi |
Shear Strength | 0.600 - 128 MPa | 87.0 - 18600 psi |
Izod Impact | 16.0 - 3300 J | 11.8 - 2430 ft-lb |
| 20.0 - 120 J @Temperature -30.0 - -30.0 °C | 14.8 - 88.5 ft-lb @Temperature -22.0 - -22.0 °F |
Izod Impact, Notched | 0.0298 - 19.2 J/cm | 0.0558 - 36.0 ft-lb/in |
| 0.350 - 0.742121 J/cm @Temperature -30.0 - -30.0 °C | 0.656 - 1.39030 ft-lb/in @Temperature -22.0 - -22.0 °F |
Izod Impact, Unnotched | 0.120 J/cm - NB | 0.225 ft-lb/in - NB |
| 15.0 - 99.99 J/cm @Temperature -30.0 - -30.0 °C | 28.1 - 187.3 ft-lb/in @Temperature -22.0 - -22.0 °F |
Izod Impact, Notched (ISO) | 2.00 kJ/m² - NB | 0.952 ft-lb/in² - NB |
| 2.00 kJ/m² - NB @Temperature -40.0 - -30.0 °C | 0.952 ft-lb/in² - NB @Temperature -40.0 - -22.0 °F |
| 5.00 - 5.00 kJ/m² @Temperature -30.0 - -30.0 °C | 2.38 - 2.38 ft-lb/in² @Temperature -22.0 - -22.0 °F |
| 5.00 - 5.00 kJ/m² @Thickness 4.00 - 4.00 mm | 2.38 - 2.38 ft-lb/in² @Thickness 0.157 - 0.157 in |
Izod Impact, Unnotched (ISO) | 5.00 kJ/m² - NB | 2.38 ft-lb/in² - NB |
| 13.0 kJ/m² - NB @Temperature -40.0 - -30.0 °C | 6.19 ft-lb/in² - NB @Temperature -40.0 - -22.0 °F |
| NB - NB @Temperature -30.0 - -30.0 °C | NB - NB @Temperature -22.0 - -22.0 °F |
| NB - NB @Thickness 3.00 - 3.00 mm | NB - NB @Thickness 0.118 - 0.118 in |
Charpy Impact Unnotched | 0.0110 J/cm² - NB | 0.0524 ft-lb/in² - NB |
| 1.40 J/cm² - NB @Temperature -30.0 - -30.0 °C | 6.66 ft-lb/in² - NB @Temperature -22.0 - -22.0 °F |
Charpy Impact, Notched | 0.200 J/cm² - NB | 0.952 ft-lb/in² - NB |
| 0.300 - 1.00 J/cm² @Temperature -30.0 - -30.0 °C | 1.43 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Gardner Impact | 2.26 - 36.0 J | 1.67 - 26.6 ft-lb |
Dart Drop, Total Energy | 2.00 - 380 J | 1.48 - 280 ft-lb |
| 88.0 - 99.0 J @Temperature -20.0 - 0.000 °C | 64.9 - 73.0 ft-lb @Temperature -4.00 - 32.0 °F |
Falling Dart Impact | 4.90 - 21.4 J | 3.61 - 15.8 ft-lb |
Instrumented Impact Total Energy | 1.48 - 38.0 J | 1.09 - 28.0 ft-lb |
Coefficient of Friction | 0.110 - 0.770 | 0.110 - 0.770 |
Coefficient of Friction, Static | 0.110 - 0.630 | 0.110 - 0.630 |
Tear Strength | 37.0 - 147 kN/m | 211 - 839 pli |
K Factor (Wear Factor) | 27.0 - 1900 | 27.0 - 1900 |
K (wear) Factor | 40.3 - 423 x 10-8 mm³/N-M | 20.0 - 210 x 10-10 in³-min/ft-lb-hr |
Limiting Pressure Velocity | 1.90 - 2.10 MPa-m/sec | 54200 - 60000 psi-ft/min |
Taber Abrasion, mg/1000 Cycles | 2.00 - 60.0 | 2.00 - 60.0 |
|
Electrical Properties | Metric | English | Comments |
---|
Electrical Resistivity | 0.0500 - 1.00e+18 ohm-cm | 0.0500 - 1.00e+18 ohm-cm |
Surface Resistance | 1.00 - 5.80e+16 ohm | 1.00 - 5.80e+16 ohm |
Static Decay | 0.0100 - 2.00 sec | 0.0100 - 2.00 sec |
Shielding Effectiveness | 50.0 - 97.0 dB | 50.0 - 97.0 dB |
Dielectric Constant | 2.52 - 6.80 | 2.52 - 6.80 |
Dielectric Strength | 4.33 - 244 kV/mm | 110 - 6200 kV/in |
Dissipation Factor | 0.000500 - 0.266 | 0.000500 - 0.266 |
Dielectric Loss Index | 0.00100 - 0.00150 | 0.00100 - 0.00150 |
Arc Resistance | 0.000 - 180 sec | 0.000 - 180 sec |
Comparative Tracking Index | 0.000 - 250 V | 0.000 - 250 V |
Hot Wire Ignition, HWI | 7.00 - 120 sec | 7.00 - 120 sec |
High Amp Arc Ignition, HAI | 0.000 - 120 arcs | 0.000 - 120 arcs |
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 150 mm/min | 0.000 - 5.91 in/min |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 2.70 - 120 µm/m-°C | 1.50 - 66.7 µin/in-°F |
| 5.00 - 60.0 µm/m-°C @Temperature 40.0 - 205 °C | 2.78 - 33.3 µin/in-°F @Temperature 104 - 401 °F |
CTE, linear, Transverse to Flow | 5.00 - 130 µm/m-°C | 2.78 - 72.2 µin/in-°F |
| 62.5 - 62.5 µm/m-°C @Temperature 40.0 - 120 °C | 34.7 - 34.7 µin/in-°F @Temperature 104 - 248 °F |
Specific Heat Capacity | 1.10 - 6.28 J/g-°C | 0.263 - 1.50 BTU/lb-°F |
Thermal Conductivity | 0.0360 - 11.0 W/m-K | 0.250 - 76.3 BTU-in/hr-ft²-°F |
Melting Point | 171 - 254 °C | 340 - 490 °F |
Maximum Service Temperature, Air | 70.0 - 300 °C | 158 - 572 °F |
Hot Ball Pressure Test | 75.0 - 125 °C | 167 - 257 °F |
Transformation Temperature, Tg | 168 - 200 °C | 334 - 392 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 116 - 237 °C | 240 - 459 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 47.2 - 393 °C | 117 - 739 °F |
Vicat Softening Point | 75.0 - 242 °C | 167 - 468 °F |
Minimum Service Temperature, Air | -50.0 - 0.000 °C | -58.0 - 32.0 °F |
Glass Transition Temp, Tg | 180 - 220 °C | 356 - 428 °F |
UL RTI, Electrical | 105 - 180 °C | 221 - 356 °F |
UL RTI, Mechanical with Impact | 105 - 180 °C | 221 - 356 °F |
UL RTI, Mechanical without Impact | 105 - 180 °C | 221 - 356 °F |
Flammability, UL94 | HB - 5VA | HB - 5VA |
Smoke Density | 0.000 - 10.0 | 0.000 - 10.0 |
Oxygen Index | 44.0 - 54.0 % | 44.0 - 54.0 % |
Glow Wire Test | 825 - 960 °C | 1520 - 1760 °F |
|
Optical Properties | Metric | English | Comments |
---|
Transmission, Visible | 58.0 - 90.0 % | 58.0 - 90.0 % |
|
Processing Properties | Metric | English | Comments |
---|
Processing Temperature | 60.0 - 410 °C | 140 - 770 °F |
Nozzle Temperature | 173 - 421 °C | 343 - 790 °F |
Adapter Temperature | 270 - 335 °C | 518 - 635 °F |
Die Temperature | 260 - 360 °C | 500 - 680 °F |
Melt Temperature | 107 - 427 °C | 225 - 801 °F |
Head Temperature | 290 - 360 °C | 554 - 680 °F |
Mold Temperature | 37.8 - 399 °C | 100 - 750 °F |
Drying Temperature | 60.0 - 152 °C | 140 - 305 °F |
Moisture Content | 0.0200 - 0.0400 % | 0.0200 - 0.0400 % |
Dew Point | -28.9 °C | -20.0 °F |
Injection Pressure | 82.7 - 124 MPa | 12000 - 18000 psi |
Vent Depth | 0.00250 - 0.00760 cm | 0.000984 - 0.00299 in |
Precipitation Temperature | 60.0 - 120 °C | 140 - 248 °F |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.