MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M 9086 High Performance Double Coated Tapes with Adhesive 375
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Tapes with 3M™ Adhesive 375 provides a high level of adhesive peel and shear performance. The adhesive system used on these products provides good adhesion to both high and low surface energy substrates. The excellent initial tack ensures that a bond of good integrity is achieved soon after application

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 3.00 milLiner Caliper
 7.50 milTotal Thickness
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 4.25 pliHDPE, 180° Peel, 2-mil Al Backing; ASTM D3330
 7.4375 pliHigh Pressure Laminate, 180° Peel, 2-mil Al Backing; ASTM D3330
 8.5625 pliABS, 180° Peel, 2-mil Al Backing; ASTM D3330
 9.125 pliStainless Steel, 180° Peel, 2-mil Al Backing; ASTM D3330
 9.125 pliGlass, 180° Peel, 2-mil Al Backing; ASTM D3330
 10.125 pliPolycarbonate, 180° Peel, 2-mil Al Backing; ASTM D3330
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 85.0 °CContinuous
 120 °CShort Term
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Adhesive CarrierTissue
Adhesive TypeModified Acrylic
AppearanceTranslucent
 White Paper (Glassine) with Black 3M Logo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
SEKISUI SPI KYDEX® XD03 Thermoplastic
Corning Iris™ Display Glass
Borosilicate Glass

PMM33321 / 168068

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.