MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SEKISUI SPI KYDEX® XD03 Thermoplastic
Categories: Polymer; Thermoplastic

Material Notes: Integral pearlescent sheet for flat lamination and membrane pressed application

KYDEX® XD03 is a proprietary, high performance thermoplastic sheet specifically formulated to meet aesthetic effect for the design needs of the building and retail interiors industry. Integrally pearlescent, this sheet is perfect for use with LED lighting or on its own.

KYDEX® XD03: (XD), superior impact, membrane pressable thermoplastic 3D laminate with integral pearlescent color. While providing good definition, it surpasses vinyl overlays, high pressure laminates and melamine in resistance to surface and edge impact. For flat lamination and membrane processing.

Suggested Applications

  • Store fixtures
  • Cabinetry
  • Workstations
  • Tabletops
  • Wainscot
  • Kiosks
  • Door and drawer fascias
  • Gondolas
  • Transaction surfaces
  • Flat laminated panels
  • Checkout counters
  • Exhibits and displays
  • Pedestals and stands
  • Logo and trademark panels

Features:

  • Highlighted in a collection of 32 developed colors, color matching also available
  • Available in P-K texture and thicknesses 0.76 mm (0.030 in) to 1.02 mm (0.040 in)
  • Easy to clean with aggressive cleaners and citrus-based cleaners (avoid ammoniated cleaners)
  • Crisp detail, minimal rejects
  • Can be formed on all standard presses and cut on all standard die-cutting machines
  • Secondary operations including machining, sawing, blanking, punching, etc. are easily performed

Values based upon 0.75 mm (0.030 in) sheet unless otherwise specified.

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Impact >= 3.0>= 3.0m; Resistance to Impact by Large Diameter Ball; EN 438-2:21
 >= 90>= 90N; Resistance to Impact by Small Diameter Ball; EN 438-2:20
 >= 1075>= 1075mm; Dart Impact Resistance; NEMA LD3.9
Abrasion 3.03.0Diamond Scratch Resistance; NEMA LD3.7
 5050g; Linear Glass Scratch Resistance; NEMA LD3.7
 
Descriptive Properties
Ball Test>3000 mmNEMA LD3.8; Impact Resistance
Boiling Water ResistanceΔ Thickness: 8.2%EN 438-2:12
 Δ Weight: 1.2%EN 438-2:12
 Grade 4EN 438-2:12
 Severe EffectNEMA LD3.5
Cleanability/Stain ResistanceAcetone: Grade 1EN 438-2:26
 Coffee: Grade 5EN 438-2:26
 Hydrogen Peroxide: Grade 5EN 438-2:26
 No EffectNEMA LD3.4
 Shoe Polish: Grade 5EN 438-2:26
 Sodium Hydroxide: Grade 5EN 438-2:26
Dimensional ChangeMD: 0.26%NEMA LD3.11
 TD: 0.39%NEMA LD3.11
Dimensional StabilityMD: 0%EN 428-2:18; Ambient Temperature
 MD: 0.07%NEMA LD3.12
 MD: -0.23%EN 438-2:17; Elevated Temperature
 TD: 0%EN 428-2:18; Ambient Temperature
 TD: 0.02%EN 438-2:17; Elevated Temperature
 TD: 0.03%NEMA LD3.12
FlammabilityB1 (0.76 mm)DIN 4102; Fire Behavior of Building Materials and Elements
 B2 (1.02 mm)DIN 4102; Fire Behavior of Building Materials and Elements
 Class 0 (0.76 mm)BS 476:6; Fire Propagation for Products
 M1 (0.76 mm + 1.02 mm)NF P 92-501; Epiradiateur Flammability (M-Classification Test)
Heat Resistance46 secNEMA LD3.10; Radiant, Coil
 47 secNEMA LD3.10; Radiant, Strip
 Grade 5EN 428-2:16; Dry Heat
High Temperature ResistanceModerate EffectNEMA LD3.6
Light ResistanceSevere EffectNEMA LD3.3
Resistance to Cigarette BurnsGrade 1EN 438-2:30
Resistance to Cracking Under StressGrade 5EN 438-2:23
Resistance to CrazingGrade 5EN 438-2:24
Resistance to ScratchingGrade 5En435-2:25
Resistance to Water VaporGrade 2EN 428-2:14
Substrate Protection against Water VaporGrade 1EN 43802:13
Surface Burning CharacteristicsClass 1 (0.76 mm + 1.02 mm)BS 476:7; Surface Spread of Flame
 Class 1/DASTM E84; of Building Materials; 1.02 mm (0.040 in) sheet
Wear Resistance1600 cyclesNEN 438-2:10; Surface Wear
 3700 cyclesNEMA LD3.13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SEKISUI SPI KYDEX® 410 ABS/PVC
SEKISUI SPI KYDEX® 6513 Thermoplastic
SEKISUI SPI KYDEX® FST2 Thermoplastic
SEKISUI SPI KYDEX® 110 Polymer Alloy Sheet
SEKISUI SPI KYDEX® 100 Polymer Alloy Sheet

PSEKIS051 / 185876

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.