MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Corning Iris™ Display Glass
Categories: Ceramic; Glass; Optical

Material Notes: Features outstanding transmission and minimal color shift, delivering bright displays with rich, accurate colors. Iris Glass is a glass light-guide plate (LGP) for edge-lit LCD TVs. Due to its intrinsic rigidity and dimensional stability, it outperforms plastic and allows TV manufacturers to significantly reduce set thickness and create TVs with slimmer bezels.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.40 g/cc0.0867 lb/in³
Moisture Absorption <= 0.00100 %<= 0.00100 %
Thickness 700 microns27.6 mil
 1100 microns43.3 mil
 1500 microns59.1 mil
 2000 microns78.7 mil
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity >= 68.0 GPa>= 9860 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 µm/m-°C4.44 µin/in-°F
Specific Heat Capacity  0.890 J/g-°C
@Temperature 50.0 °C
0.213 BTU/lb-°F
@Temperature 122 °F
 0.950 J/g-°C
@Temperature 100 °C
0.227 BTU/lb-°F
@Temperature 212 °F
Thermal Conductivity  1.20 W/m-K
@Temperature 50.0 °C
8.33 BTU-in/hr-ft²-°F
@Temperature 122 °F
 1.20 W/m-K
@Temperature 100 °C
8.33 BTU-in/hr-ft²-°F
@Temperature 212 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.49
@Wavelength 633 nm
1.49
@Wavelength 633 nm
Transmission, Visible  86 %
@Thickness 500 mm,
Wavelength 700 nm
86 %
@Thickness 19.7 in,
Wavelength 700 nm
Long path; Excludes Fresnel reflections
 90 %
@Thickness 500 mm,
Wavelength 625 nm
90 %
@Thickness 19.7 in,
Wavelength 625 nm
Long path; Excludes Fresnel reflections
 90 %
@Wavelength 450 nm,
Thickness 500 mm
90 %
@Wavelength 450 nm,
Thickness 19.7 in
Long path; Excludes Fresnel reflections
 92 %
@Wavelength 400 nm,
Thickness 500 mm
92 %
@Wavelength 400 nm,
Thickness 19.7 in
Long path; Excludes Fresnel reflections
 94 %
@Thickness 500 mm,
Wavelength 500 nm
94 %
@Thickness 19.7 in,
Wavelength 500 nm
Long path; Excludes Fresnel reflections

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Corning Gorilla® Glass 4 Touch Screen Glass
Borosilicate Glass
Corning Gorilla® Glass 5 Display Glass
Corning Eagle XG® Slim Display Glass
E-Glass Fiber, Generic

CCORNG990 / 197395

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.