MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AISI 94B15 Steel
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 9000 Series Steel; Low Alloy Steel; Carbon Steel; Low Carbon Steel

Key Words: UNS G94151, AMS 6275 A, ASTM A519, SAE J404, SAE J770
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.87 g/ccfield average for steels
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 163 - 202hot rolled and cold drawn
Hardness, Knoop 204Converted from Brinell
Hardness, Rockwell B 89Converted from Brinell
Hardness, Vickers 192Converted from Brinell
Modulus of Elasticity 200 GPaEstimated
Bulk Modulus 160 GPaTypical for steel.
Poissons Ratio 0.29Calculated
Machinability 70 %hot rolled and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPaTypical for steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000174 ohm-cmEstimated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.5 µm/m-°C
@Temperature 20.0 °C
 12.2 µm/m-°C
@Temperature 250 °C
Estimated
 13.9 µm/m-°C
@Temperature 500 °C
 14.7 µm/m-°C
@Temperature 1000 °C
Specific Heat Capacity 0.472 J/g-°CEstimated
Thermal Conductivity 51.9 W/m-KTypical steel
 
Component Elements PropertiesOriginal ValueComments
Boron, B 0.00050 - 0.0030 %
Carbon, C 0.13 - 0.18 %
Chromium, Cr 0.30 - 0.50 %
Iron, Fe 97.192 - 98.2895 %As remainder
Manganese, Mn 0.75 - 1.0 %
Molybdenum, Mo 0.080 - 0.15 %
Nickel, Ni 0.30 - 0.60 %
Phosphorus, P <= 0.035 %
Silicon, Si 0.15 - 0.30 %
Sulfur, S <= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 94B15H Steel
AISI 94B17 Steel
AISI 94B17H Steel
AISI 1023 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 8720 Steel

M941AA / 8707

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.