MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI 1023 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: Similar to AISI 1020 steel, responds well to heat treating and cold work. Fair machinability and weldability. Excellent cold formability.

Key Words: UNS G10230
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.858 g/cc0.2839 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 121121
Hardness, Knoop 140140Converted from Brinell
Hardness, Rockwell B 6868Converted from Brinell
Hardness, Vickers 126126Converted from Brinell
Tensile Strength, Ultimate 425 MPa61600 psi
Tensile Strength, Yield 360 MPa52200 psi
Elongation at Break 15 %15 %In 50 mm
Reduction of Area 40 %40 %
Modulus of Elasticity 205 GPa29700 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.290.29Typical For Steel
Machinability 65 %65 %Based on AISI 1212 steel = 100%
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000169 ohm-cm
@Temperature 20.0 °C
0.0000169 ohm-cm
@Temperature 68.0 °F
 0.0000219 ohm-cm
@Temperature 100 °C
0.0000219 ohm-cm
@Temperature 212 °F
 0.0000292 ohm-cm
@Temperature 200 °C
0.0000292 ohm-cm
@Temperature 392 °F
 0.0000487 ohm-cm
@Temperature 400 °C
0.0000487 ohm-cm
@Temperature 752 °F
 0.0000758 ohm-cm
@Temperature 600 °C
0.0000758 ohm-cm
@Temperature 1110 °F
 0.0000925 ohm-cm
@Temperature 700 °C
0.0000925 ohm-cm
@Temperature 1290 °F
 0.0001094 ohm-cm
@Temperature 800 °C
0.0001094 ohm-cm
@Temperature 1470 °F
 0.0001136 ohm-cm
@Temperature 900 °C
0.0001136 ohm-cm
@Temperature 1650 °F
 0.0001167 ohm-cm
@Temperature 1000 °C
0.0001167 ohm-cm
@Temperature 1830 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.1 µm/m-°C
@Temperature 0.000 - 100 °C
6.72 µin/in-°F
@Temperature 32.0 - 212 °F
 13.3 µm/m-°C
@Temperature 0.000 - 300 °C
7.39 µin/in-°F
@Temperature 32.0 - 572 °F
 14.4 µm/m-°C
@Temperature 0.000 - 500 °C
8.00 µin/in-°F
@Temperature 32.0 - 932 °F
Specific Heat Capacity 0.486 J/g-°C0.116 BTU/lb-°F50-100ºC
Thermal Conductivity 51.9 W/m-K
@Temperature 0.000 °C
360 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.19 - 0.25 %0.19 - 0.25 %
Iron, Fe 99.06 - 99.51 %99.06 - 99.51 %As remainder
Manganese, Mn 0.30 - 0.60 %0.30 - 0.60 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1023 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1025 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1020 Steel, cold rolled
AISI 1018 Steel, cold drawn
AISI 1022 Steel, cold drawn round (19 - 32 mm)

M1023A / 6875

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.