System Message
Advertise with MatWeb!
Data sheets for over
185,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Material Category Search
User Input Problem
Find a Material Category:
Select a Material Category:
Carbon (866 matls)
Ceramic (10004 matls)
Fluid (7562 matls)
Metal (17052 matls)
Other Engineering Material (8063 matls)
Polymer (97635 matls)
Pure Element (507 matls)
Wood and Natural Products (398 matls)
Selected Material Category:
Search Results
There are
1612
materials in the category
Low Carbon Steel
. If your material is not listed, please refer to our
search strategy
page for assistance in limiting your search.
Found
1612
Results
-- Page
1
2
3
4
5
6
7
8
9
10
11
12
13
14
15
16
17
18
19
20
of
33
--
[Prev Page]
[Next Page]
-- view
25
50
75
100
150
200
per page
Use Folder
Contains
New Folder Name
My Folder
Select
Material Name
1
Overview of materials for Low Carbon Steel
2
AISI 1005 Steel
3
AISI 1006 Steel, cold drawn
4
AISI 1006 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round
5
AISI 1006 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round
6
AISI 1006 Steel, CQ, DQ, and DQSK sheet, 1.6-5.8 (0.06-0.23 in) mm thick
7
AISI 1008 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round
8
AISI 1008 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round
9
AISI 1008 Steel, CQ, DQ, and DQSK sheet, 1.6-5.8 mm thick
10
AISI M1008 Merchant Quality Carbon Steel, Composition Spec
11
AISI 1009 Steel
12
AISI 1010 Steel, cold drawn
13
AISI 1010 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round or thickness
14
AISI 1010 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round or thickness
15
AISI 1010 Steel, CQ sheet,1.6-5.8 mm round or thickness
16
AISI M1010 Merchant Quality Carbon Steel, Composition Spec
17
AISI 1012 Steel, cold drawn
18
AISI 1012 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round or thickness
19
AISI 1012 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round or thickness
20
AISI 1012 Steel, CQ sheet,1.6-5.8 mm round or thickness
21
AISI M1012 Merchant Quality Carbon Steel, Composition Spec
22
AISI 1013 Carbon Steel Composition Spec
23
AISI 1015 Steel, cold drawn
24
AISI 1015 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
25
AISI 1015 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
26
AISI 1015 Steel, as rolled
27
AISI 1015 Steel, normalized at 925°C (1700°F)
28
AISI 1015 Steel, annealed at 870°C (1600°F)
29
AISI 1015 Steel, annealed at 870°C (1600°F), furnace cooled 17°C (31°F) per hour to 725°C (1340°F), air cooled, 25 mm (1 in.) round
30
AISI 1015 Steel, normalized at 925°C (1700°F), 13 mm (0.5 in.) round
31
AISI 1015 Steel, normalized at 925°C (1700°F), 25 mm (1 in.) round
32
AISI 1015 Steel, normalized at 925°C (1700°F), 50 mm (2 in.) round
33
AISI 1015 Steel, normalized at 925°C (1700°F), 100 mm (4 in.) round
34
AISI 1015 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 13 mm (0.5 in.) round
35
AISI 1015 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 25 mm (1 in.) round
36
AISI 1015 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 50 mm (2 in.) round
37
AISI 1015 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 100 mm (4 in.) round
38
AISI M1015 Merchant Quality Carbon Steel, Composition Spec
39
AISI 1016 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
40
AISI 1016 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
41
AISI 1017 Steel, cold drawn
42
AISI 1017 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
43
AISI M1017 Merchant Quality Carbon Steel, Composition Spec
44
AISI 1018 Steel, cold drawn
45
AISI 1018 Steel, hot rolled, quenched, and tempered
46
AISI 1018 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
47
AISI 1018 Steel, cold drawn, quenched, and tempered, 19-32 mm (0.75-1.25 in) round
48
AISI 1018 Steel, as cold drawn, 16-22 mm (0.625-0.875 in) round
49
AISI 1018 Steel, as cold drawn, 22-32 mm (0.875-1.25 in) round
50
AISI 1018 Steel, as cold drawn, 32-50 mm (1.25-2 in) round
Found
1612
Results
-- Page
1
2
3
4
5
6
7
8
9
10
11
12
13
14
15
16
17
18
19
20
of
33
--
[Prev Page]
[Next Page]
-- view
25
50
75
100
150
200
per page
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Instructions:
This page allows you to quickly access all of the polymers/plastics, metals, ceramics, fluids, and other engineering materials in the MatWeb material property database. Just select the material category you would like to find from the tree. Click on the [+] icon to open subcategory branches in the tree. Then click the
'Find'
button next to its box. You can then follow the links to the most complete data sheets on the Web, with information on over 1000 available properties, including dielectric constant, Poisson's ratio, glass transition temperature, dissipation factor, and Vicat softening point.
Proto3000 - Rapid Prototyping
Notes:
Visit MatWeb's
property-based search page
to limit your results to materials that meet specific property performance criteria.
Text searches can be done from any page - use the
Quick Search
box in the top right of the page.
More
Search Strategies
on how to find information in MatWeb.
Show All Materials
- an inefficient drill-down to data sheets. Registered users who are logged in omit a step in this drill down process.
Top
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2026 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.