MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI 1023 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: Machinability and weldability are fair. Cold formability of these steels is good to excellent. This grade responds favorably to heat treating and cold work.

Key Words: UNS G10230, ASTM A29, ASTM A510, ASTM A575, ASTM A576, ASTM A659, SAE J403, JIS S 22 C, JIS S 20 CK, SAE J412, SAE J414, DIN 1.1151, AFNOR XC 18 S, AFNOR XC 25, JIS S 20 C
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.858 g/cc0.2839 lb/in³Chemical composition of 0.23% C, 0.635% Mn, 0.11% Si, annealed at 925°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 111111
Hardness, Knoop 129129Converted from Brinell
Hardness, Rockwell B 6464Converted from Brinell
Hardness, Vickers 115115Converted from Brinell
Tensile Strength, Ultimate 385 MPa55800 psi
Tensile Strength, Yield 215 MPa31200 psi
Elongation at Break 25 %25 %
Reduction of Area 50 %50 %
Modulus of Elasticity 200 GPa29000 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.290.29Typical For Steel
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000169 ohm-cm
@Temperature 20.0 °C
0.0000169 ohm-cm
@Temperature 68.0 °F
 0.0000219 ohm-cm
@Temperature 100 °C
0.0000219 ohm-cm
@Temperature 212 °F
 0.0000292 ohm-cm
@Temperature 200 °C
0.0000292 ohm-cm
@Temperature 392 °F
 0.0000487 ohm-cm
@Temperature 400 °C
0.0000487 ohm-cm
@Temperature 752 °F
 0.0000758 ohm-cm
@Temperature 600 °C
0.0000758 ohm-cm
@Temperature 1110 °F
 0.0000925 ohm-cm
@Temperature 700 °C
0.0000925 ohm-cm
@Temperature 1290 °F
 0.0001094 ohm-cm
@Temperature 800 °C
0.0001094 ohm-cm
@Temperature 1470 °F
 0.0001136 ohm-cm
@Temperature 900 °C
0.0001136 ohm-cm
@Temperature 1650 °F
 0.0001167 ohm-cm
@Temperature 1000 °C
0.0001167 ohm-cm
@Temperature 1830 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.1 µm/m-°C
@Temperature 20.0 - 100 °C
6.72 µin/in-°F
@Temperature 68.0 - 212 °F
 12.8 µm/m-°C
@Temperature 20.0 - 200 °C
7.11 µin/in-°F
@Temperature 68.0 - 392 °F
 13.3 µm/m-°C
@Temperature 20.0 - 300 °C
7.39 µin/in-°F
@Temperature 68.0 - 572 °F
 13.9 µm/m-°C
@Temperature 20.0 - 400 °C
7.72 µin/in-°F
@Temperature 68.0 - 752 °F
 14.4 µm/m-°C
@Temperature 20.0 - 500 °C
8.00 µin/in-°F
@Temperature 68.0 - 932 °F
 14.8 µm/m-°C
@Temperature 20.0 - 600 °C
8.22 µin/in-°F
@Temperature 68.0 - 1110 °F
Specific Heat Capacity  0.486 J/g-°C
@Temperature >=100 °C
0.116 BTU/lb-°F
@Temperature >=212 °F
 0.519 J/g-°C
@Temperature 150 - 200 °C
0.124 BTU/lb-°F
@Temperature 302 - 392 °F
 0.532 J/g-°C
@Temperature 200 - 250 °C
0.127 BTU/lb-°F
@Temperature 392 - 482 °F
 0.557 J/g-°C
@Temperature 250 - 300 °C
0.133 BTU/lb-°F
@Temperature 482 - 572 °F
 0.574 J/g-°C
@Temperature 300 - 350 °C
0.137 BTU/lb-°F
@Temperature 572 - 662 °F
 0.599 J/g-°C
@Temperature 350 - 400 °C
0.143 BTU/lb-°F
@Temperature 662 - 752 °F
 0.662 J/g-°C
@Temperature 450 - 500 °C
0.158 BTU/lb-°F
@Temperature 842 - 932 °F
 0.749 J/g-°C
@Temperature 550 - 600 °C
0.179 BTU/lb-°F
@Temperature 1020 - 1110 °F
 0.846 J/g-°C
@Temperature 650 - 700 °C
0.202 BTU/lb-°F
@Temperature 1200 - 1290 °F
 0.950 J/g-°C
@Temperature 750 - 800 °C
0.227 BTU/lb-°F
@Temperature 1380 - 1470 °F
 1.432 J/g-°C
@Temperature 700 - 750 °C
0.3423 BTU/lb-°F
@Temperature 1290 - 1380 °F
Thermal Conductivity  26.1 W/m-K
@Temperature 800 °C
181 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 27.2 W/m-K
@Temperature 1000 °C
189 BTU-in/hr-ft²-°F
@Temperature 1830 °F
 29.8 W/m-K
@Temperature 1200 °C
207 BTU-in/hr-ft²-°F
@Temperature 2190 °F
 31.8 W/m-K
@Temperature 700 °C
221 BTU-in/hr-ft²-°F
@Temperature 1290 °F
 35.6 W/m-K
@Temperature 600 °C
247 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 39.4 W/m-K
@Temperature 500 °C
273 BTU-in/hr-ft²-°F
@Temperature 932 °F
 42.7 W/m-K
@Temperature 400 °C
296 BTU-in/hr-ft²-°F
@Temperature 752 °F
 46.0 W/m-K
@Temperature 300 °C
319 BTU-in/hr-ft²-°F
@Temperature 572 °F
 49.0 W/m-K
@Temperature 200 °C
340 BTU-in/hr-ft²-°F
@Temperature 392 °F
 51.2 W/m-K
@Temperature 100 °C
355 BTU-in/hr-ft²-°F
@Temperature 212 °F
 51.9 W/m-K
@Temperature 0.000 °C
360 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.19 - 0.25 %0.19 - 0.25 %
Iron, Fe 99.06 - 99.51 %99.06 - 99.51 %As remainder
Manganese, Mn 0.30 - 0.60 %0.30 - 0.60 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1023 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1016 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1020 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1025 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1026 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round

M1023B / 6876

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.