MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI 1023 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: Machinability and weldability are fair. Cold formability of these steels is good to excellent. This grade responds favorably to heat treating and cold work.

Key Words: UNS G10230, ASTM A29, ASTM A510, ASTM A575, ASTM A576, ASTM A659, SAE J403, JIS S 22 C, JIS S 20 CK, SAE J412, SAE J414, DIN 1.1151, AFNOR XC 18 S, AFNOR XC 25, JIS S 20 C
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.858 g/ccChemical composition of 0.23% C, 0.635% Mn, 0.11% Si, annealed at 925°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 111
Hardness, Knoop 129Converted from Brinell
Hardness, Rockwell B 64Converted from Brinell
Hardness, Vickers 115Converted from Brinell
Tensile Strength, Ultimate 385 MPa
Tensile Strength, Yield 215 MPa
Elongation at Break 25 %
Reduction of Area 50 %
Modulus of Elasticity 200 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel
Poissons Ratio 0.29Typical For Steel
Shear Modulus 80.0 GPaTypical for steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000169 ohm-cm
@Temperature 20.0 °C
 0.0000219 ohm-cm
@Temperature 100 °C
 0.0000292 ohm-cm
@Temperature 200 °C
 0.0000487 ohm-cm
@Temperature 400 °C
 0.0000758 ohm-cm
@Temperature 600 °C
 0.0000925 ohm-cm
@Temperature 700 °C
 0.0001094 ohm-cm
@Temperature 800 °C
 0.0001136 ohm-cm
@Temperature 900 °C
 0.0001167 ohm-cm
@Temperature 1000 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.1 µm/m-°C
@Temperature 20.0 - 100 °C
 12.8 µm/m-°C
@Temperature 20.0 - 200 °C
 13.3 µm/m-°C
@Temperature 20.0 - 300 °C
 13.9 µm/m-°C
@Temperature 20.0 - 400 °C
 14.4 µm/m-°C
@Temperature 20.0 - 500 °C
 14.8 µm/m-°C
@Temperature 20.0 - 600 °C
Specific Heat Capacity 0.486 J/g-°C
@Temperature >=100 °C
 0.519 J/g-°C
@Temperature 150 - 200 °C
 0.532 J/g-°C
@Temperature 200 - 250 °C
 0.557 J/g-°C
@Temperature 250 - 300 °C
 0.574 J/g-°C
@Temperature 300 - 350 °C
 0.599 J/g-°C
@Temperature 350 - 400 °C
 0.662 J/g-°C
@Temperature 450 - 500 °C
 0.749 J/g-°C
@Temperature 550 - 600 °C
 0.846 J/g-°C
@Temperature 650 - 700 °C
 0.950 J/g-°C
@Temperature 750 - 800 °C
 1.432 J/g-°C
@Temperature 700 - 750 °C
Thermal Conductivity 26.1 W/m-K
@Temperature 800 °C
 27.2 W/m-K
@Temperature 1000 °C
 29.8 W/m-K
@Temperature 1200 °C
 31.8 W/m-K
@Temperature 700 °C
 35.6 W/m-K
@Temperature 600 °C
 39.4 W/m-K
@Temperature 500 °C
 42.7 W/m-K
@Temperature 400 °C
 46.0 W/m-K
@Temperature 300 °C
 49.0 W/m-K
@Temperature 200 °C
 51.2 W/m-K
@Temperature 100 °C
 51.9 W/m-K
@Temperature 0.000 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.19 - 0.25 %
Iron, Fe 99.06 - 99.51 %As remainder
Manganese, Mn 0.30 - 0.60 %
Phosphorus, P <= 0.040 %
Sulfur, S <= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1023 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1016 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1020 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1025 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1026 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round

M1023B / 6876

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.