Material Category Search
User Input Problem
Find a Material Category:
Select a Material Category:
Carbon (866 matls)
Ceramic (10004 matls)
Fluid (7562 matls)
Metal (17052 matls)
Other Engineering Material (8063 matls)
Polymer (97635 matls)
Pure Element (507 matls)
Wood and Natural Products (398 matls)
Selected Material Category:
Search Results
There are
118
materials in the category
AISI 9000 Series Steel
. If your material is not listed, please refer to our
search strategy
page for assistance in limiting your search.
Found
118
Results
-- Page
1
2
3
of
3
--
[Prev Page]
[Next Page]
-- view
25
50
75
100
150
200
per page
Use Folder
Contains
New Folder Name
My Folder
Select
Material Name
1
Overview of materials for AISI 9000 Series Steel
2
SAE 9254 Low Alloy Steel, Spheroidized Annealed and Cold Drawn Bar
3
AISI 9255 Steel, normalized at 900°C (1650°F)
4
AISI 9255 Steel, annealed at 845°C (1550°F)
5
AISI 9255 Steel, annealed at 845°C (1550°F), 25 mm (1 in.) round
6
AISI 9255 Steel, normalized at 900°C (1650°F), 13 mm (0.5 in.) round
7
AISI 9255 Steel, normalized at 900°C (1650°F), 25 mm (1 in.) round
8
AISI 9255 Steel, normalized at 900°C (1650°F), 50 mm (2 in.) round
9
AISI 9255 Steel, normalized at 900°C (1650°F), 100 mm (4 in.) round
10
AISI 9255 Steel, oil quenched from 885°C (1625°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
11
AISI 9255 Steel, oil quenched from 885°C (1625°F), 540°C (1000°F) temper, 25 mm (1 in.) round
12
AISI 9255 Steel, oil quenched from 885°C (1625°F), 540°C (1000°F) temper, 50 mm (2 in.) round
13
AISI 9255 Steel, oil quenched from 885°C (1625°F), 540°C (1000°F) temper, 100 mm (4 in.) round
14
AISI 9255 Steel, oil quenched from 885°C (1625°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
15
AISI 9255 Steel, oil quenched from 885°C (1625°F), 595°C (1100°F) temper, 25 mm (1 in.) round
16
AISI 9255 Steel, oil quenched from 885°C (1625°F), 595°C (1100°F) temper, 50 mm (2 in.) round
17
AISI 9255 Steel, oil quenched from 885°C (1625°F), 595°C (1100°F) temper, 100 mm (4 in.) round
18
AISI 9255 Steel, oil quenched from 885°C (1625°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
19
AISI 9255 Steel, oil quenched from 885°C (1625°F), 650°C (1200°F) temper, 25 mm (1 in.) round
20
AISI 9255 Steel, oil quenched from 885°C (1625°F), 650°C (1200°F) temper, 50 mm (2 in.) round
21
AISI 9255 Steel, oil quenched from 885°C (1625°F), 650°C (1200°F) temper, 100 mm (4 in.) round
22
AISI 9261 Steel (UNS G92610)
23
AISI 9260 Steel
24
AISI 9260H Steel
25
AISI E9310 Steel, direct quenched from pot, tempered at 150°C (300°F), 0.99 mm case depth
26
AISI E9310 Steel, single quenched and tempered at 150°C (300°F), 1.2 mm case depth
27
AISI E9310 Steel, double quenched and tempered at 150°C (300°F), 1.4 mm case depth
28
AISI E9310 Steel, direct quenched from pot, tempered at 230°C (450°F), 0.99 mm case depth
29
AISI E9310 Steel, single quenched and tempered at 230°C (450°F), 1.2 mm case depth
30
AISI E9310 Steel, double quenched and tempered at 230°C (450°F), 1.4 mm case depth
31
AISI E9310 Steel, annealed at 845°C (1550°F), 25 mm (1 in.) round
32
AISI E9310 Steel, normalized at 890°C (1635°F), 13 mm (0.5 in.) round
33
AISI E9310 Steel, normalized at 890°C (1635°F), 25 mm (1 in.) round
34
AISI E9310 Steel, normalized at 890°C (1635°F), 50 mm (2 in.) round
35
AISI E9310 Steel, normalized at 890°C (1635°F), 100 mm (4 in.) round
36
AISI E9310 Steel, mock carburized, 790°C (1450°F) reheat, 150°C (300°F) temper, 13 mm (0.5 in.) round
37
AISI E9310 Steel, mock carburized, 790°C (1450°F) reheat, 150°C (300°F) temper, 25 mm (1 in.) round
38
AISI E9310 Steel, mock carburized, 790°C (1450°F) reheat, 150°C (300°F) temper, 50 mm (2 in.) round
39
AISI E9310 Steel, mock carburized, 790°C (1450°F) reheat, 150°C (300°F) temper, 100 mm (4 in.) round
40
AISI E9310 Steel, mock carburized, 790°C (1450°F) reheat, 230°C (450°F) temper, 13 mm (0.5 in.) round
41
AISI E9310 Steel, mock carburized, 790°C (1450°F) reheat, 230°C (450°F) temper, 25 mm (1 in.) round
42
AISI E9310 Steel, mock carburized, 790°C (1450°F) reheat, 230°C (450°F) temper, 50 mm (2 in.) round
43
AISI E9310 Steel, mock carburized, 790°C (1450°F) reheat, 230°C (450°F) temper, 100 mm (4 in.) round
44
AISI E9310 Steel, normalized at 890°C (1635°F)
45
AISI E9310 Steel, annealed at 845°C (1550°F)
46
AISI E9310 Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, 775°C (1430°F) reheat, 150°C (300°F) temper
47
AISI E9310 Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, 800°C (1470°F) reheat, 150°C (300°F) temper
48
AISI E9310 Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, 830°C (1525°F) reheat, 150°C (300°F) temper
49
AISI E9310 Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, 150°C (300°F) temper
50
AISI E9310 Steel, normalized, machined to 13.7 mm rounds, pseudocarburized, 775°C (1430°F) reheat, 150°C (300°F) temper
Found
118
Results
-- Page
1
2
3
of
3
--
[Prev Page]
[Next Page]
-- view
25
50
75
100
150
200
per page
Instructions:
This page allows you to quickly access all of the polymers/plastics, metals, ceramics, fluids, and other engineering materials in the MatWeb material property database. Just select the material category you would like to find from the tree. Click on the [+] icon to open subcategory branches in the tree. Then click the
'Find'
button next to its box. You can then follow the links to the most complete data sheets on the Web, with information on over 1000 available properties, including dielectric constant, Poisson's ratio, glass transition temperature, dissipation factor, and Vicat softening point.
Proto3000 - Rapid Prototyping
Notes:
Visit MatWeb's
property-based search page
to limit your results to materials that meet specific property performance criteria.
Text searches can be done from any page - use the
Quick Search
box in the top right of the page.
More
Search Strategies
on how to find information in MatWeb.
Show All Materials
- an inefficient drill-down to data sheets. Registered users who are logged in omit a step in this drill down process.
Top
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.