MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trelleborg Emerson & Cuming Eccobond® 26 Two-Component General Purpose Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Emerson & Cuming 26 Eccobond® Two-Component General Purpose Epoxy Adhesive
Filled, room temperature curing, general purpose, epoxy adhesive. Recommended for varied uses including repair and manufacture of tools, furniture, boats, and electronic sub-assemblies. Mix Ratio of 100:100. Bonding Type: Epoxy

The Eccobond® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 14.5 MPa2100 psi
 
Processing PropertiesMetricEnglishComments
Cure Time  19.8 min
@Temperature 65.0 °C
0.330 hour
@Temperature 149 °F
 240 min
@Temperature 25.0 °C
4.00 hour
@Temperature 77.0 °F
 
Descriptive Properties
ColorOff-white
ViscosityThixotropic Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Adhesive
Hexcel® HexPly® 954-2A Curing Cyanate Resin
Coastal Enterprises EP-76 Epoxy Bonding Adhesive
Atom Adhesives AA-SUPERTHERM 195 Epoxy Adhesive
Atom Adhesives AA-DUCT N02 Epoxy Adhesive

PEMERS45 / 35737

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.