MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® eXten D238 V30 Nylon 6,10, 30% glass fiber, Conditioned
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610); Nylon 610, Glass Reinforced

Material Notes: Description: TECHNYL® eXten D 238 V30 is a PA6,10 30% glass fiber reinforced and impact modified suitable for injection molding. TECHNYL® eXten D 238 V30 is based on a partially bio-sourced polyamide 6,10. This material is available in black.

Available in: Asia Pacific, Europe, Latin America and North America

Product Applications: TECHNYL® eXten D 238 V30 is suitable to the manufacturing of injection molded parts in all sectors of applications. It offers excellent chemical resistance, low water absorption, very good mechanical properties and moldability.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccISO 1183/A
Linear Mold Shrinkage, Flow 0.051 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.079 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPaISO 527 Type 1A
Elongation at Break 9.0 %ISO 527 Type 1A
Tensile Modulus 4900 MPaISO 527 Type 1A
Charpy Impact Unnotched 10.0 J/cm²ISO 179/1eU
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® eXten D238 V30 Nylon 6,10, 30% glass fiber, DRY
BASF Ultramid® S3WG6 Balance 30% Glass Filled PA 610 (Dry)
BASF Ultramid® S3WG6 Balance 30% Glass Filled PA 610 (Conditioned)
Domo TECHNYL® A 216 S30 PA66, 30% glass spheres, DRY
Arkema Rilsamid® AZM 30 O TLD PA12-GF30

PRHOD554 / 137785

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.