MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 216 S30 PA66, 30% glass spheres, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Description: Polyamide 66, reinforced with 30% of glass spheres, for injection molding.

Available in: Europe

Product Applications: TECHNYL® A 216 S30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is recommended for mechanical components which require a very good surface finish with low warpage, and good compression strength. This product is available in natural, black, grey, red, white, and in special colors on request

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183/A
Water Absorption 0.75 %
@Temperature 23.0 °C,
Time 86400 sec
0.75 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inIsotropy
Linear Mold Shrinkage, Flow 0.016 cm/cm0.016 in/in
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psiISO 527 Type 1A
Elongation at Break 9.0 %9.0 %ISO 527 Type 1A
Elongation at Yield 4.0 %4.0 %ISO 527 type 1 A
Tensile Modulus 4.50 GPa653 ksiISO 527 Type 1A
Flexural Strength 135 MPa19600 psiISO 178
Flexural Modulus 3.85 GPa558 ksiISO 178
Izod Impact, Notched (ISO) 2.50 kJ/m²1.19 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 0.350 J/cm²1.67 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+14 ohm-cm5.00e+14 ohm-cmIEC 60093
Surface Resistance 5.00e+14 ohm5.00e+14 ohmIEC 60093
Dielectric Strength 30.0 kV/mm762 kV/inIEC 60243
Dissipation Factor 0.0200.020IEC 60250
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 6.00 µm/m-°C
@Temperature 23.0 - 85.0 °C
3.33 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 263 °C505 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75/Af
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
ISO 1210
 
Processing PropertiesMetricEnglishComments
Feed Temperature 270 - 280 °C518 - 536 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone275-285°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Iupilon® CFH 2030 Polycarbonate
Domo TECHNYL® A 216 PA66, DRY
Domo Technyl® C216V15 15% Glass Filled Nylon 6
Domo Technyl® C216V25 25% Glass Filled Nylon 6
Domo TECHNYL® eXten D238 V30 Nylon 6,10, 30% glass fiber, Conditioned

PRHOD596 / 137827

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.