MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® eXten D238 V30 Nylon 6,10, 30% glass fiber, DRY
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610); Nylon 610, Glass Reinforced

Material Notes: Description: TECHNYL® eXten D 238 V30 is a PA6,10 30% glass fiber reinforced and impact modified suitable for injection molding. TECHNYL® eXten D 238 V30 is based on a partially bio-sourced polyamide 6,10. This material is available in black.

Available in: Asia Pacific, Europe, Latin America and North America

Product Applications: TECHNYL® eXten D 238 V30 is suitable to the manufacturing of injection molded parts in all sectors of applications. It offers excellent chemical resistance, low water absorption, very good mechanical properties and moldability.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ISO 1183/A
Water Absorption 0.34 %
@Time 86400 sec
0.34 %
@Time 24.0 hour
ISO 64
Water Absorption at Saturation 1.9 %1.9 %ISO 64
Linear Mold Shrinkage, Flow 0.051 cm/cm0.051 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.079 cm/cm0.079 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7878ISO 868
Tensile Strength at Break 115 MPa16700 psiISO 527 Type 1A
Elongation at Break 4.0 %4.0 %ISO 527 Type 1A
Tensile Modulus 7.90 GPa1150 ksiISO 527 Type 1A
Charpy Impact Unnotched  8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 10.0 J/cm²
@Temperature -30.0 °C
47.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 215 - 220 °C419 - 428 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 194 °C381 °FISO 75/Af
Shrinkage 0.64 %0.64 %Isotropy
 
Processing PropertiesMetricEnglishComments
Feed Temperature 250 - 290 °C482 - 554 °F
Mold Temperature 8.00 °C46.4 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.15 %<= 0.15 %
 
Descriptive Properties
Compression Zone250-290°C
Mixing Zone250-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® eXten D238 V30 Nylon 6,10, 30% glass fiber, Conditioned
Domo TECHNYL® eXten D218 V30 Nylon 6.10, 30% glass fiber, DRY
BASF Ultramid® S3WG6 Balance 30% Glass Filled PA 610 (Dry)
BASF Ultramid® S3WG6 Balance 30% Glass Filled PA 610 (Conditioned)
Domo TECHNYL® A 216 S30 PA66, 30% glass spheres, DRY

PRHOD553 / 137784

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.