MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials PEARLTHANE® 11H94 Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: PEARLTHANE® D11H94 is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring adequate hardness as well as excellent flow and mechanical properties, including an outstandingly low compression set value. Product recommended for injection molding applications with an extremely short cycle time. PEARLTHANE® D11H94 is especially recommended for injection molding applications such as: automotive parts, seals and gaskets and a variety of high performance technical parts.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccISO 2781
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95ISO 868
Tensile Strength, Yield 6102 psiISO 527-2/5A/500
Elongation at Break 515 %ISO 527-2/5A/500
50% Modulus 10.0 MPa
@Strain 50 %
ISO 527-2/5A/500
100% Modulus 1.743 ksi
@Strain 100 %
ISO 527-2/5A/500
300% Modulus 3.341 ksi
@Strain 300 %
ISO 527-2/5A/500
Tear Strength 771 plinicked; ISO 34-1B
Abrasion 35Resistance (mm³); ISO 4649-A
Compression Set 32 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 37 %
@Temperature 70.0 °C,
Time 252000 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 127 °CISO 306 (A50)
 
Processing PropertiesOriginal ValueComments
Feed Temperature 210 °C
Nozzle Temperature 225 °C
Zone 1 215 °C
Zone 2 225 °C
Zone 3 225 °C
Zone 4 225 °C
Drying Temperature 100 °C
Dry Time 3.00 - 4.00 hour
Dew Point -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 11T93 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU

PMES36 / 88413

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.