Vacuum formed products are rigid, self-supporting fiber insulation manufactured from a slurry of ceramic fibers, binders and other proprietary ingredients. Customers are provided with optimized, engineered solutions from our wide range of formulations. Kaowool PM is a thin, lightweight product that is manufactured to close tolerances with an excellent surface finish and good thermal properties.Information provided by Morgan Advanced Materials |