Physical Properties | Metric | English | Comments |
---|
Density | 0.0640 - 0.160 g/cc | 0.00231 - 0.00578 lb/in³ |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength | 0.0300 MPa | 4.35 psi |
| 0.0700 MPa | 10.2 psi |
| 0.0900 MPa | 13.1 psi |
| 0.110 MPa | 16.0 psi |
|
Thermal Properties | Metric | English | Comments |
---|
Specific Heat Capacity | 1.13 J/g-°C @Temperature 1090 °C | 0.270 BTU/lb-°F @Temperature 1990 °F |
Thermal Conductivity | 0.0600 W/m-K @Temperature 200 °C | 0.416 BTU-in/hr-ft²-°F @Temperature 392 °F |
| 0.0600 W/m-K @Temperature 200 °C | 0.416 BTU-in/hr-ft²-°F @Temperature 392 °F |
| 0.0700 W/m-K @Temperature 200 °C | 0.486 BTU-in/hr-ft²-°F @Temperature 392 °F |
| 0.0900 W/m-K @Temperature 400 °C | 0.625 BTU-in/hr-ft²-°F @Temperature 752 °F |
| 0.100 W/m-K @Temperature 400 °C | 0.694 BTU-in/hr-ft²-°F @Temperature 752 °F |
| 0.110 W/m-K @Temperature 400 °C | 0.763 BTU-in/hr-ft²-°F @Temperature 752 °F |
| 0.120 W/m-K @Temperature 400 °C | 0.833 BTU-in/hr-ft²-°F @Temperature 752 °F |
| 0.130 W/m-K @Temperature 600 °C | 0.902 BTU-in/hr-ft²-°F @Temperature 1110 °F |
| 0.150 W/m-K @Temperature 600 °C | 1.04 BTU-in/hr-ft²-°F @Temperature 1110 °F |
| 0.160 W/m-K @Temperature 600 °C | 1.11 BTU-in/hr-ft²-°F @Temperature 1110 °F |
| 0.180 W/m-K @Temperature 800 °C | 1.25 BTU-in/hr-ft²-°F @Temperature 1470 °F |
| 0.200 W/m-K @Temperature 800 °C | 1.39 BTU-in/hr-ft²-°F @Temperature 1470 °F |
| 0.200 W/m-K @Temperature 600 °C | 1.39 BTU-in/hr-ft²-°F @Temperature 1110 °F |
| 0.230 W/m-K @Temperature 800 °C | 1.60 BTU-in/hr-ft²-°F @Temperature 1470 °F |
| 0.250 W/m-K @Temperature 1000 °C | 1.74 BTU-in/hr-ft²-°F @Temperature 1830 °F |
| 0.270 W/m-K @Temperature 1000 °C | 1.87 BTU-in/hr-ft²-°F @Temperature 1830 °F |
| 0.300 W/m-K @Temperature 800 °C | 2.08 BTU-in/hr-ft²-°F @Temperature 1470 °F |
| 0.320 W/m-K @Temperature 1000 °C | 2.22 BTU-in/hr-ft²-°F @Temperature 1830 °F |
| 0.430 W/m-K @Temperature 1000 °C | 2.98 BTU-in/hr-ft²-°F @Temperature 1830 °F |
Shrinkage | 1.5 % @Temperature 1000 °C, Time 86400 sec | 1.5 % @Temperature 1830 °F, Time 24.0 hour |
| 2.2 % @Temperature 1100 °C, Time 86400 sec | 2.2 % @Temperature 2010 °F, Time 24.0 hour |
| 3.0 % @Temperature 1200 °C, Time 86400 sec | 3.0 % @Temperature 2190 °F, Time 24.0 hour |
| 5.5 % @Temperature 1300 °C, Time 86400 sec | 5.5 % @Temperature 2370 °F, Time 24.0 hour |
|
Component Elements Properties | Metric | English | Comments |
---|
Al2O3 | 44 % | 44 % |
CaO+MgO | 0.050 % | 0.050 % |
K2O+Na2O | 0.10 % | 0.10 % |
Other | 0.15 % | 0.15 % |
SiO2 | 56 % | 56 % |
|
Descriptive Properties |
---|
Classification Temperature (°C) | 1260 |
Color | white |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.