MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Kaowool HD Organic RCF Vacuum Formed Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Vacuum formed products are rigid, self-supporting fiber insulation manufactured from a slurry of ceramic fibers, binders and other proprietary ingredients. Customers are provided with optimized, engineered solutions from our wide range of formulations. Kaowool HD is a high strength product recommended for tough mechanical stress areas.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0260 g/cc0.000939 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00103 - 0.00121 GPa0.149 - 0.175 ksi
Compressive Strength 0.340 - 0.480 MPa49.3 - 69.6 psiat 5% deformation
 0.480 - 0.620 MPa69.6 - 89.9 psiat 10% deformation
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0900 W/m-K
@Temperature 260 °C
0.625 BTU-in/hr-ft²-°F
@Temperature 500 °F
ASTM C201
 0.120 W/m-K
@Temperature 538 °C
0.833 BTU-in/hr-ft²-°F
@Temperature 1000 °F
ASTM C201
 0.160 W/m-K
@Temperature 816 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 1500 °F
ASTM C201
 0.230 W/m-K
@Temperature 1093 °C
1.60 BTU-in/hr-ft²-°F
@Temperature 1999 °F
ASTM C201
Maximum Service Temperature, Air 1260 °C2300 °FContinuous Use
 1316 °C2401 °F
Shrinkage  0.10 %
@Temperature 816 °C,
Time 86400 sec
0.10 %
@Temperature 1500 °F,
Time 24.0 hour
 1.4 %
@Temperature 982 °C,
Time 86400 sec
1.4 %
@Temperature 1800 °F,
Time 24.0 hour
 2.5 %
@Temperature 1093 °C,
Time 86400 sec
2.5 %
@Temperature 1999 °F,
Time 24.0 hour
 2.8 %
@Temperature 1204 °C,
Time 86400 sec
2.8 %
@Temperature 2199 °F,
Time 24.0 hour
 
Component Elements PropertiesMetricEnglishComments
Al2O3 41 %41 %
CaO+MgO 5.0 %5.0 %
Loss on Ignition(%) 5.0 - 8.0 %5.0 - 8.0 %
Other 4.0 - 7.0 %4.0 - 7.0 %organic
SiO2 53 %53 %
 
Descriptive Properties
Colorbeige

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Cerablanket™ Thermal Ceramic
Morgan Advanced Ceramics Ceramic Fiber Board S Board Ceramic Fibre Board
Morgan Advanced Ceramics Kaowool Ceramic Felt 1260 Thermal Ceramic
Morgan Advanced Ceramics Kaowool PM Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics MAFTEC Blanket

CMORF70116 / 203414

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.