MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Reade Advanced Materials Wollastonite (CaSiO3 or CaO.SiO2)
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Description: A white to yellowish-brown naturally occurring mineral. It has good strength, firing characteristics and ability to reduce crazing. Used as a source of silica and alkalis in the production of ceramics. Used to produce wall tiles, semivitreous bodies, ceramic insulators and glazes, reinforced thermoplastics, adhesives, and ceramic-bonded abrasives.
Forms Available: Various granulations are available. Primarily 10 X 100 mesh, 200 mesh X down and 325 mesh X down

Information provided by Reade Advanced Materials.

Key Words: CaSiO3, CaO.SiO2, Calcium metasilicate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.80 - 2.90 g/cc2.80 - 2.90 g/cc
pH 9.0 - 109.0 - 10aqueous solution
Molecular Weight 116 g/mol116 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 4.5 - 5.04.5 - 5.020°C
 
Thermal PropertiesMetricEnglishComments
Melting Point 1540 °C2800 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.631.63
 
Descriptive Properties
Colorwhite
Crystal Structureacicular

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Accuratus MACOR Machinable Glass Ceramic
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC
Bostik Big Tile & Stone™ Latex-Modified Mortar
Bostik D-2001® Ultra-Premium™ Ceramic Tile Mastic
Bostik Glass-Mate™ Glass Tile Mortar

CREADE021 / 1955

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.