MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Bostik Glass-Mate™ Glass Tile Mortar
Categories: Other Engineering Material

Material Notes: Description: Bostik Glass-Mate™ is a premium, polymer-modified, thin-set mortar that exhibits superior bond strength, durability, nonsag properties and workability. Its bright white color and high polymer content make it ideal for setting individual glass tiles, sheet mounted glass tile, and most types of tile or natural stone in thin-set applications over cement-based or masonry substrates..

Key Features:

  • For installing mosaic and glass tile
  • Bright white enhances glass tile appearance
  • Mix with Bostik 425™ additive for submerged tile installations

Information provided by Bostik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatile Organic Compounds (VOC) Content 0.050 g/l0.050 g/lwhen mixed with water; SCAQMD Rule #1168
 0.26 g/l0.26 g/lwhen mixed with Bostik 425 Additive; SCAQMD Rule #1168
 
Mechanical PropertiesMetricEnglishComments
Shear Strength >= 1.03 MPa>= 150 psiBond when mixed with Bostik 425 Admixture; Exceeds ANSI A118.4
 >= 1.03 MPa>= 150 psiBond when mixed with Bostik 425 Admixture; Exceeds ANSI A118.11
 >= 1.38 MPa>= 200 psiBond when mixed with Bostik 425 Admixture; Exceeds ANSI A118.4
 >= 2.07 MPa>= 300 psiBond when mixed with Bostik 425 Admixture; Exceeds ANSI A118.4
 >= 1.03 MPa
@Time 2.42e+6 sec
>= 150 psi
@Time 672 hour
Mortar to Quarry Tile; ANSI A118.4
 >= 1.03 MPa
@Time 2.42e+6 sec
>= 150 psi
@Time 672 hour
Quarry Tile to Plywood; ANSI A118.11
 >= 1.38 MPa
@Time 2.42e+6 sec
>= 200 psi
@Time 672 hour
Mortar to Porcelain Mosaic Tile; ANSI A118.4
 >= 2.07 MPa
@Time 2.42e+6 sec
>= 300 psi
@Time 672 hour
Mortar to Glazed Wall Tile; ANSI A118.4
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourGrouting with Cement Based Grouts
 1440 - 2880 min24.0 - 48.0 hourGrouting with Bostik Urethane Grouts
 2880 min48.0 hourGrouting with Bostik 1900 Epoxy Grout
 2880 min48.0 hourGrouting with Bostik EzPoxyTM 100% Solids Epoxy Grout
 10100 min168 hourHeavy Traffic, Frost or Rain
 30200 min504 hourWater Submersion (When mixed with Bostik 425™ Additive instead of water)
Pot Life <= 120 min<= 120 min
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorBright white
Installation Temperature10-35°C
Recycled Content1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bostik Tube & Tile Caulk Siliconized-Acrylic Caulk
Bostik Professional Grade™ Ceramic Tile Mastic
Bostik D-2001® Ultra-Premium™ Ceramic Tile Mastic
Bostik Big Tile & Stone™ Latex-Modified Mortar
MarkeTech Repton 868 Zirconia + 8 mol% Yttria (YSZ)

PBOSTK012 / 191548

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.