MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bostik D-2001® Ultra-Premium™ Ceramic Tile Mastic
Categories: Polymer; Adhesive; Thermoset

Material Notes: Description: Bostik D-2001® Ultra-Premium™ Mastic is a high performance adhesive for the interior installation of all types of ceramic and stone tile (except moisture sensitive marble). Bostik D-2001® Ultra-Premium™ Mastic is ready to use for a fast, professional installation and provides excellent vertical grab for large bodied tiles. Bostik D-2001® Ultra-Premium™ Mastic exceeds the requirements of ANSI A136.1 Type I and II.

Key Features:

  • Exceeds ANSI A136.1, Type I & Type II
  • Fast, professional installation
  • Excellent for large format ceramic tiles on floors & walls

Information provided by Bostik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.56 g/cc0.0563 lb/in³
Volatile Organic Compounds (VOC) Content 1.0 g/l1.0 g/l
 
Mechanical PropertiesMetricEnglishComments
Shear Strength >= 0.345 MPa>= 50.0 psiWet
 >= 3.79 MPa>= 550 psiDry
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 93.3 °C>= 200 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 - 2880 min24.0 - 48.0 hour
Shelf Life 12.0 Month
@Temperature 1.67 - 37.8 °C
12.0 Month
@Temperature 35.0 - 100 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bostik Professional Grade™ Ceramic Tile Mastic
Bostik Glass-Mate™ Glass Tile Mortar
Bostik Big Tile & Stone™ Latex-Modified Mortar
Bostik Tube & Tile Caulk Siliconized-Acrylic Caulk
MarkeTech Repton 868 Zirconia + 8 mol% Yttria (YSZ)

PBOSTK002 / 191538

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.