MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bostik Big Tile & Stone™ Latex-Modified Mortar
Categories: Other Engineering Material

Material Notes: Description: Big Tile & Stone™ is a latex-modified, medium bed mortar used for interior or exterior installations to set all large sized ceramic, porcelain, granite, slate, marble, limestone, and dimension stone tiles. Use over properly prepared concrete; structurally-sound, exterior grade plywood (interior/dry use only); cementitious backer board; Bostik® Ultra-Set® Advanced; Bostik® Black-Top™; Bostik® GoldPlus™; and existing, well-bonded vinyl/VCT or ceramic tile. Big Tile & Stone may also be used as a leveling bed to compensate for uneven tile and stone thickness; smooth irregular or uneven substrates; or to minimize lippage.

Information provided by Bostik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 23.4 MPa
@Time 2.42e+6 sec
3400 psi
@Time 672 hour
Shear Strength  1.72 MPa
@Time 2.42e+6 sec
250 psi
@Time 672 hour
Quarry to Wood; ANSI REQ 150
 2.07 MPa
@Time 2.42e+6 sec
300 psi
@Time 672 hour
Quarry Tile
 2.59 MPa
@Time 2.42e+6 sec
375 psi
@Time 672 hour
Porcelain Tile; ANSI REQ 200
 3.84 MPa
@Time 2.42e+6 sec
557 psi
@Time 672 hour
Glazed Wall Tile; ANSI REQ 300
 
Processing PropertiesMetricEnglishComments
Cure Time 480 - 600 min8.00 - 10.0 hourInitial Set
 600 - 900 min10.0 - 15.0 hourFinal Set
Pot Life 60.0 - 120 min60.0 - 120 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bostik Tube & Tile Caulk Siliconized-Acrylic Caulk
Bostik Professional Grade™ Ceramic Tile Mastic
Bostik Glass-Mate™ Glass Tile Mortar
Bostik D-2001® Ultra-Premium™ Ceramic Tile Mastic
MarkeTech Repton 868 Zirconia + 8 mol% Yttria (YSZ)

PBOSTK019 / 191555

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.