Description: LUPOY NF 1009F08R, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transparency and impact strength and exhibits excellent processing characteristics. Main Characteristics: Good mold release, Medium viscosity, Non chlorine, bromine, nor phosphate additives and Complying with global environmental standards Applications: Lighting, TV Housing, Electrons/Electrical and Information Technology Equipment CAS: 103598-77-2 Information provided by LG Chemical |