Flame retardant and mold release grade with normal fluidity, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications. Applications: Electric, electronic and business machine components that need flame retardancy.Information provided by Teijin Chemicals Ltd. |