MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical Lupoy NF1007F 10R Polycarbonate Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Description: LUPOY NF 1007F10R, eco-friendly UL94 V0/3.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transparency and impact strength and exhibits excellent processing characteristics.

Main Characteristics: Good mold release, Medium viscosity, Non chlorine, bromine, nor phosphate additives and Complying with global environmental standards

Applications: Lighting, TV Housing, Electrons/Electrical and Information Technology Equipment

CAS: 103598-77-2

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Water Absorption 0.15 %
@Temperature 23.0 °C,
Time 86400 sec
0.15 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Moisture Absorption at Equilibrium 0.32 %
@Temperature 23.0 °C
0.32 %
@Temperature 73.4 °F
50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm0.00050 - 0.00070 in/inASTM D955
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7373ASTM D785
Tensile Strength, Ultimate 71.0 MPa10300 psiASTM D638
Tensile Strength, Yield 60.0 MPa8700 psi50mm/min; ASTM D638
Elongation at Break 150 %150 %ASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Tensile Modulus 2.41 GPa350 ksiASTM D638
Flexural Yield Strength 96.0 MPa13900 psiASTM D790
Flexural Modulus 2.41 GPa350 ksiASTM D790
Izod Impact, Notched 9.074 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
17.00 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm notch; ASTM D256
Izod Impact, Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256
Dart Drop, Total Energy 87.0 J
@Thickness 3.20 mm
64.2 ft-lb
@Thickness 0.126 in
203m/min; ASTM D3763
Abrasion 45
@Load 1.00 kg
45
@Load 2.20 lb
[%], CS-10 F wheel, 500 cycles; ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+17 ohm-cm2.00e+17 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 60 Hz
3.0
@Frequency 60 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm432 kV/inASTM D149
Dissipation Factor 0.0010
@Frequency 60.0 Hz
0.0010
@Frequency 60.0 Hz
ASTM D150
Arc Resistance 0.00 - 60 sec0.00 - 60 secASTM D495
Comparative Tracking Index 250 V
@Thickness 2.00 mm
250 V
@Thickness 0.0787 in
IEC 112
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness >=1.50 mm
15 - 30 sec
@Thickness >=0.0591 in
 30 - 60 sec
@Thickness >=3.00 mm
30 - 60 sec
@Thickness >=0.118 in
High Amp Arc Ignition, HAI  >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
 >= 120 arcs
@Thickness 3.00 mm
>= 120 arcs
@Thickness 0.118 in
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/min
 
Thermal PropertiesMetricEnglishComments
CTE, linear 68.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F
@Temperature -40.0 - 180 °F
ASTM D696
Hot Ball Pressure Test >= 125 °C>= 257 °FIEC 598-1
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
@Thickness 4.00 mm
280 °F
@Thickness 0.157 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
@Thickness 4.00 mm
259 °F
@Thickness 0.157 in
Unannealed; ASTM D648
Vicat Softening Point 146 °C
@Load 5.10 kg
295 °F
@Load 11.2 lb
50°C/hr; ASTM D1525
Softening Point 150 - 200 °C302 - 392 °Fmelting point per MSDS
UL RTI, Electrical  130 °C
@Thickness >=0.750 mm
266 °F
@Thickness >=0.0295 in
 130 °C
@Thickness >=1.50 mm
266 °F
@Thickness >=0.0591 in
 130 °C
@Thickness >=3.00 mm
266 °F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact  110 °C
@Thickness >=0.750 mm
230 °F
@Thickness >=0.0295 in
 110 °C
@Thickness >=1.50 mm
230 °F
@Thickness >=0.0591 in
 110 °C
@Thickness >=3.00 mm
230 °F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact  130 °C
@Thickness >=0.750 mm
266 °F
@Thickness >=0.0295 in
 130 °C
@Thickness >=1.50 mm
266 °F
@Thickness >=0.0591 in
 130 °C
@Thickness >=3.00 mm
266 °F
@Thickness >=0.118 in
Flammability, UL94  V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
ASTM D635
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
ASTM D635
Flash Point >= 450 °C>= 842 °F
Oxygen Index 35 %35 %ASTM D2863
Glow Wire Test 850 °C
@Thickness 2.00 mm,
Time 5.00 sec
1560 °F
@Thickness 0.0787 in,
Time 0.00139 hour
IEC 695-2-1
Ignition Temperature >= 450 °C>= 842 °FAutoignition
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ASTM D542
Haze 0.70 - 1.5 %0.70 - 1.5 %ASTM D1003
Transmission, Visible 89 %89 %ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical Lupoy NF1005F 03R Polycarbonate Resin
LG Chemical Lupoy NF1009F 08R Polycarbonate Resin
LG Chemical LUPOY EF1006F PC, Halogen Free, Flame Retardant, High Heat Resistance
Trinseo EMERGE™ 4630-10 Polycarbonate
Trinseo CALIBRE™ 302V-6 Polycarbonate Resin

PLAY694 / 148704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.