MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: PEARLTHANE® 16N95UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis and microbial resistance. It can be both extruded and injection-molded.

PEARLTHANE® 16N95UV when extruded, can be used for making (pneumatic) tubes, profiles and cables. When processed by injection molding, can be used for technical parts.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 21.6 kg
10 g/10 min
@Load 47.6 lb
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9494ASTM D2240
Tensile Strength, Yield 40.0 MPa5800 psiASTM D412
Elongation at Break 575 %575 %ASTM D412
100% Modulus 11.00 MPa
@Strain 100 %
1595 psi
@Strain 100 %
ASTM D412
300% Modulus 16.00 MPa
@Strain 300 %
2321 psi
@Strain 300 %
ASTM D412
Tear Strength 130 kN/m742 pliASTM D624 (Die C)
Abrasion 4040loss (mm³); DIN 53.516
Compression Set  30 %
@Temperature 23.0 °C,
Time 252000 sec
30 %
@Temperature 73.4 °F,
Time 70.0 hour
ASTM D395B
 44 %
@Temperature 70.0 °C,
Time 86400 sec
44 %
@Temperature 158 °F,
Time 24.0 hour
ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 - 188 °C352 - 370 °FMQSA 111
Glass Transition Temp, Tg -31.1 °C-24.0 °FDSC, 50°F/10min; ISO 11357-2
 
Processing PropertiesMetricEnglishComments
Feed Temperature 200 °C392 °F
Nozzle Temperature 210 °C410 °F
Zone 1 180 - 195 °C356 - 383 °F
Zone 2 190 - 210 °C374 - 410 °F
Zone 3 200 - 220 °C392 - 428 °F
Zone 4 190 - 210 °C374 - 410 °F
Die Temperature 185 - 195 °C365 - 383 °F
Mold Temperature 35.0 °C95.0 °F
Moisture Content <= 0.10 %<= 0.10 %MQSA 44
Screw Speed 50 rpm50 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 11T60D Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU

PMES61A / 109237

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.