Coating Description: SHS 8000 TWAS is a glass forming iron based alloy that forms a nanocomposite comprised of a mixed amorphous and nanoscale microstructure when sprayed as a coating. SHS 8000 features high wear resistance, elevated temperature erosion resistance and a unique high hardness/toughness combination.Key Performance Characteristics- Excels in elevated temperature environments where fly ash and bed ash erosion occurs
- Superior bond strength without necessity of bond coat
- Hardness increases as a function of time and temperature
Application Process: Twin Wire Arc Spraying (TWAS) Information Provided by The NanoSteel Company, Inc. |