System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Goodfellow Iron 77.5/Boron 15/Silicon 7.5 Alloy
Categories:
Metal
;
Ferrous Metal
;
Superalloy
;
Iron Base
Material Notes:
Metallic glasses (glassy alloys) or amorphous metals. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.
Information provided by Goodfellow.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Metric
English
Comments
Vickers Microhardness
940
940
kg(f)/mm²
Elongation at Break
2.3 %
2.3 %
Tensile Modulus
155
GPa
22500
ksi
Electrical Properties
Metric
English
Comments
Electrical Resistivity
0.000124
ohm-cm
0.000124
ohm-cm
Curie Temperature
422
°C
792
°F
Thermal Properties
Metric
English
Comments
CTE, linear
8.70
µm/m-°C
@Temperature 20.0 °C
4.83
µin/in-°F
@Temperature 68.0 °F
Crystallization Temperature
553
°C
1030
°F
Component Elements Properties
Metric
English
Comments
Boron, B
15 %
15 %
Iron, Fe
77.5 %
77.5 %
Silicon, Si
7.5 %
7.5 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel (Extended Electro-Magnetic Data)
The NanoSteel® Company SHS 8000 TWAS Iron Based Alloy, Cored Wire
Goodfellow Iron 40/Nickel 38/Boron 18 Alloy
Goodfellow Cobalt/Silicon/Boron/Iron/Nickel Alloy
NGOODF157 / 16229
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.