MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Goodfellow Nickel/Iron/Silicon/Boron Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Solder/Braze Alloy

Material Notes: Metallic glass (glassy alloy) or amorphous metal. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.40 g/cc0.267 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 800800kg(f)/mm²
Tensile Strength at Break 1500 - 2000 MPa218000 - 290000 psi
Tensile Modulus 150 GPa21800 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000135 ohm-cm0.000135 ohm-cm
Magnetic Coercive Force, Hc 0.0126 Oe0.0126 Oe
Magnetic Saturation Flux Density, Bmax 8000 Gauss8000 Gauss
Magnetic Remanence, Br <= 1.0 Gauss<= 1.0 GaussRemanence Ratio, Br/Bs
Curie Temperature 260 °C500 °F
 
Thermal PropertiesMetricEnglishComments
Crystallization Temperature 450 °C842 °F
Maximum Service Temperature, Air 120 °C248 °F
 
Component Elements PropertiesMetricEnglishComments
Iron, Fe 40 %40 %
Molybdenum, Mo 1.0 - 2.0 %1.0 - 2.0 %
Nickel, Ni 40 %40 %
Silicon, Si 19 %19 %Si + B content = 19 wt%
 
Descriptive Properties
Saturation magnetostriction (x10^-6)8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow Iron 77.5/Boron 15/Silicon 7.5 Alloy
Goodfellow Iron 40/Nickel 38/Boron 18 Alloy
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel (Extended Electro-Magnetic Data)
Carpenter Hiperco® Alloy 50 Fe-Co-V Soft Magnetic Alloy, Cold Rolled

NGOODF188 / 16258

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.